Nimonic 90 is a high-performance, nickel-based superalloy primarily composed of nickel, chromium, and titanium, designed for exceptional strength, oxidation resistance, and long-term thermal stability. A service temperature range extending to 950°C is especially suitable for components subjected to high mechanical stresses and corrosive environments, including gas turbines, power generation, and aerospace applications. The alloy's unique combination of alloying elements, such as aluminum, titanium, and molybdenum, provides excellent creep resistance and oxidation resistance at elevated temperatures.
Due to its excellent mechanical properties, Nimonic 90 is often processed through CNC machining services to meet the exacting demands of aerospace, power generation, and nuclear industries. This processing method is ideal for achieving the tight tolerances required in turbine blades, combustion chambers, and other critical components. Furthermore, CNC machining ensures high precision in parts subjected to extreme environments, providing structural integrity and long-lasting performance.
Nimonic 90 (UNS N07090 / W.Nr. 2.4632 / AMS 5586) is a precipitation-hardened superalloy, strengthened by forming gamma prime (γ′) precipitates. This enhances the alloy's strength, creep resistance, and thermal stability, especially in applications involving extended exposure to high temperatures.
Element | Composition Range (wt.%) | Key Role |
|---|---|---|
Nickel (Ni) | Balance (≥55.0) | Provides thermal stability and base matrix strength |
Chromium (Cr) | 19.0–22.0 | Enhances oxidation and hot corrosion resistance |
Cobalt (Co) | 15.0–20.0 | Increases creep and fatigue resistance |
Molybdenum (Mo) | 4.0–6.0 | Solid solution strengthening and carbide formation |
Titanium (Ti) | 2.0–2.6 | Forms Ni₃Ti gamma-prime precipitates |
Aluminum (Al) | 1.0–1.5 | Enhances γ′ phase hardening for high-temperature strength |
Iron (Fe) | ≤2.0 | Residual element |
Carbon (C) | ≤0.10 | Improves creep strength via carbide precipitation |
Manganese (Mn) | ≤1.0 | Improves hot working characteristics |
Silicon (Si) | ≤1.0 | Aids in oxidation resistance |
Sulfur (S) | ≤0.015 | Controlled to avoid hot cracking during machining and welding |
Property | Value (Typical) | Test Standard/Condition |
|---|---|---|
Density | 8.65 g/cm³ | ASTM B311 |
Melting Range | 1340–1390°C | ASTM E1268 |
Thermal Conductivity | 12.5 W/m·K at 100°C | ASTM E1225 |
Electrical Resistivity | 1.15 µΩ·m at 20°C | ASTM B193 |
Thermal Expansion | 13.5 µm/m·°C (20–1000°C) | ASTM E228 |
Specific Heat Capacity | 445 J/kg·K at 20°C | ASTM E1269 |
Elastic Modulus | 210 GPa at 20°C | ASTM E111 |
Property | Value (Typical) | Test Standard |
|---|---|---|
Tensile Strength | 1050–1200 MPa | ASTM E8/E8M |
Yield Strength (0.2%) | 760–840 MPa | ASTM E8/E8M |
Elongation | ≥15% | ASTM E8/E8M |
Hardness | 230–260 HB | ASTM E10 |
Creep Rupture Strength | 250 MPa at 850°C (1000h) | ASTM E139 |
Fatigue Resistance | Excellent | ASTM E466 |
High-Temperature Strength Retention Retains tensile strength >1050 MPa and yield strength >760 MPa at 850°C, providing reliable performance in turbine engines and other high-temperature systems.
Creep Resistance Exhibits creep rupture strength of 250 MPa at 850°C for 1000 hours, verified under ASTM E139, ensuring long-term stability in aerospace and power plant components.
Oxidation Resistance Resistant to oxidation up to 950°C, forming a stable Cr₂O₃ oxide layer that minimizes mass loss and surface degradation in high-temperature environments.
Thermal Fatigue Durability Low thermal expansion coefficient of 13.5 µm/m·°C minimizes stress buildup in components subjected to repeated heating and cooling cycles.
Enhanced Structural Stability Strengthened by both γ′ precipitates and Mo-rich carbides, improving resistance to creep and fatigue in rotating parts and fasteners exposed to high mechanical and thermal stress.
Gamma prime and other hard phases lead to rapid tool wear, especially on uncoated carbide tools.
Nimonic 90 has low thermal conductivity, leading to high cutting zone temperatures that can cause dimensional drift and thermal cracking.
The alloy rapidly work hardens, requiring precise cutting parameters and sharp tools to maintain surface finish and dimensional accuracy.
Parameter | Recommendation | Rationale |
|---|---|---|
Tool Material | Fine-grain carbide (K30), CBN inserts for finishing | High-temperature wear resistance |
Coating | AlTiN or TiSiN (3–5 µm PVD) | Protects against heat and galling |
Geometry | Positive rake, honed edge (~0.05 mm) | Lowers cutting force and vibration |
Operation | Speed (m/min) | Feed (mm/rev) | Depth of Cut (mm) | Coolant Pressure (bar) |
|---|---|---|---|---|
Roughing | 10–15 | 0.15–0.25 | 1.5–2.5 | 100–120 |
Finishing | 25–40 | 0.05–0.10 | 0.3–1.0 | 120–150 |
HIP improves fatigue strength by >20% and eliminates internal porosity. Typical processing conditions include 1100°C and 100–150 MPa for 2–4 hours, ensuring 100% densification for structural components.
Heat Treatment involves solution annealing at ~1120°C followed by aging at 850–870°C to maximize γ′ precipitation. This process improves creep resistance and dimensional stability in long-term service.
Superalloy Welding using matching filler metal (e.g., ERNiCrCoMo-1) ensures weld strength >90% of base metal and minimal cracking in pressure-retaining joints.
TBC Coating applies a 100–300 µm yttria-stabilized zirconia (YSZ) layer via APS or EB-PVD methods, reducing substrate temperatures by up to 200°C in turbine components.
EDM enables feature tolerances of ±0.005 mm on hardened sections without inducing thermal stress, ideal for cooling holes and thin-walled structures.
Deep Hole Drilling with L/D ratios >30:1 ensures straightness <0.3 mm/m and Ra <1.6 µm, suitable for cooling channels in high-temperature hardware.
Material Testing includes creep rupture validation at 850°C/1000h, XRD phase analysis, SEM microstructure review, and ultrasonic flaw detection to ASME standards.
Aerospace Turbine Engines: Turbine blades, vanes, and disk components subjected to extreme thermal and mechanical stress.
Power Generation: Combustors, transition ducts, and structural bolting in gas turbines and high-efficiency heat recovery systems.
Nuclear Energy Systems: Springs, valve internals, and spacers used in high-radiation, high-pressure reactor environments.
Automotive Performance Systems: Exhaust brackets, turbo components, and thermal shields requiring oxidation and fatigue resistance.
Industrial Heating Equipment: Retorts, radiant tubes, and heat-treating fixtures exposed to temperatures up to 1000°C.
What are the optimal CNC machining techniques to handle the hardness and abrasiveness of Nimonic 90 for high-precision parts?
How can tool wear be minimized when machining Nimonic 90 for turbine blades and other high-temperature components?
What specific heat treatment processes are recommended for Nimonic 90 to ensure maximum strength and stability at temperatures exceeding 850°C?
How does Nimonic 90 perform in CNC machining compared to other Nimonic alloys for applications like gas turbines and power plants?
What is the typical lead time for machining complex Nimonic 90 parts, such as turbine vanes or fasteners, with high tolerance requirements?