Monel 400 is a solid-solution nickel-copper alloy known for its exceptional corrosion resistance, high strength, and good weldability. With a nominal composition of 67% nickel and 30% copper, it offers outstanding performance in marine and chemical environments, particularly where resistance to acidic and alkaline media, saltwater, and hydrofluoric acid is critical.
Monel 400 maintains structural integrity from cryogenic temperatures up to 550°C and exhibits good toughness across this range. The alloy is often CNC machined in annealed condition to ensure stability and tight tolerance control for critical components such as valves, shafts, fittings, and heat exchanger parts.
Monel 400 (UNS N04400 / ASTM B164 / AMS 4675) is non-hardenable by heat treatment and relies on cold working for strengthening. It is delivered in annealed, stress-relieved, or cold-drawn condition depending on application demands.
Element | Composition Range (wt.%) | Key Role |
|---|---|---|
Nickel (Ni) | ≥63.0 | Base metal for corrosion resistance and ductility |
Copper (Cu) | 28.0–34.0 | Enhances resistance to acids and seawater |
Iron (Fe) | ≤2.5 | Strengthens the alloy without compromising corrosion resistance |
Manganese (Mn) | ≤2.0 | Improves hot workability |
Silicon (Si) | ≤0.5 | Enhances oxidation resistance |
Carbon (C) | ≤0.3 | Controlled to maintain weldability |
Sulfur (S) | ≤0.024 | Minimized to prevent hot cracking |
Property | Value (Typical) | Test Standard/Condition |
|---|---|---|
Density | 8.80 g/cm³ | ASTM B311 |
Melting Range | 1300–1350°C | ASTM E1268 |
Thermal Conductivity | 22.0 W/m·K at 100°C | ASTM E1225 |
Electrical Resistivity | 0.43 µΩ·m at 20°C | ASTM B193 |
Thermal Expansion | 13.9 µm/m·°C (20–300°C) | ASTM E228 |
Specific Heat Capacity | 427 J/kg·K at 20°C | ASTM E1269 |
Elastic Modulus | 179 GPa at 20°C | ASTM E111 |
Property | Value (Typical) | Test Standard |
|---|---|---|
Tensile Strength | 480–620 MPa | ASTM E8/E8M |
Yield Strength (0.2%) | 170–280 MPa | ASTM E8/E8M |
Elongation | ≥35% (25mm gauge) | ASTM E8/E8M |
Hardness | 120–180 HB | ASTM E10 |
Impact Toughness | Excellent at -196°C | ASTM E23 |
Excellent Corrosion Resistance: Withstands hydrofluoric acid, seawater, sulfuric acid, and alkali environments—ideal for marine and chemical process systems.
Non-Magnetic and Cryogenic Stability: Maintains toughness at sub-zero temperatures, making it suitable for liquefied gas equipment.
Good Machinability: While work-hardening, it offers stable performance during CNC turning and milling, especially with proper tooling and coolant strategies.
Weldability: Easily welded using gas tungsten arc, gas metal arc, and resistance welding methods, without post-weld cracking.
Rapid work hardening requires consistent depth of cut to avoid excessive tool wear and dimensional drift.
Prone to built-up edge (BUE), leading to surface finish degradation and unpredictable chip formation.
Generates localized heat zones at the tool-workpiece interface, especially during drilling and threading.
Parameter | Recommendation | Rationale |
|---|---|---|
Tool Material | Carbide tools or high-speed steel (HSS-Co) | Maintains sharpness and wear resistance |
Coating | TiAlN or TiCN (2–3 µm) | Reduces BUE formation and thermal stress |
Geometry | 10–12° rake with polished flutes | Enhances chip evacuation and cutting consistency |
Operation | Speed (m/min) | Feed (mm/rev) | DOC (mm) | Coolant Pressure (bar) |
|---|---|---|---|---|
Roughing | 20–35 | 0.20–0.30 | 2.0–3.0 | 50–80 |
Finishing | 40–60 | 0.05–0.15 | 0.5–1.0 | 80–120 |
HIP is rarely used for Monel 400 but can be applied to improve internal soundness in cast or additively manufactured parts.
Heat Treatment typically includes annealing at 850–900°C followed by controlled cooling to relieve residual stresses.
Superalloy Welding allows Monel 400 to be joined without cracking, using Ni-Cu filler metals (ERNiCu-7).
TBC Coating is not commonly used, but corrosion-resistant coatings may be applied for seawater or acidic service.
EDM is ideal for producing precision grooves, slots, and cavities in hardened or thin-walled Monel 400 components.
Deep Hole Drilling enables internal coolant paths or threaded bores in marine pump shafts and valve bodies.
Material Testing includes salt spray testing (ASTM B117), mechanical property verification, and grain size inspection per ASTM E112.
Pump shafts, propeller shafts, seawater valves, and fasteners.
Outstanding resistance to biofouling, salt spray, and brine environments.
Acid-handling tanks, heat exchangers, agitators, and process piping.
Performs well in hydrochloric, sulfuric, and hydrofluoric acid conditions.
Downhole tools, valves, and instrumentation exposed to sour gas.
Complies with NACE MR0175 for H₂S resistance in corrosive wells.
Fuel system components, cryogenic valves, and brackets.
Maintains strength and impact resistance at temperatures as low as −200°C.
What makes Monel 400 superior to stainless steel in marine and acidic environments?
What are the optimal feed and speed parameters for CNC machining Monel 400?
Can Monel 400 components be welded and machined without post-treatment?