हिन्दी

Rene 104

High-strength, oxidation-resistant nickel-based superalloy designed for critical aerospace and power generation components subjected to extreme temperatures. Ideal for precision CNC machining of gas turbine and combustion system components.

Introduction to Rene 104

Rene 104 is a high-performance nickel-based superalloy known for its excellent high-temperature strength, oxidation resistance, and creep resistance. Designed primarily for aerospace and power generation applications, it is ideal for components exposed to extreme mechanical and thermal loads, such as turbine blades, compressor discs, and gas turbine parts. Rene 104 provides superior strength retention and dimensional stability at temperatures exceeding 1000°C, making it one of the most reliable materials for high-efficiency turbines and engines.

Due to the demanding nature of these applications, CNC machining services are employed to produce high-precision components from Rene 104, ensuring tight tolerances and optimal performance. CNC machining offers the repeatability, precision, and reliability required for such critical parts.


Chemical, Physical, and Mechanical Properties of Rene 104

Rene 104 (UNS N07040 / W.Nr. 2.4954) is a nickel-based superalloy with a highly optimized composition designed to maximize strength, oxidation resistance, and thermal stability.

Chemical Composition (Typical)

Element

Composition Range (wt.%)

Key Role

Nickel (Ni)

Balance (~50.0)

Base matrix; provides oxidation resistance and strength at high temperatures

Chromium (Cr)

13.0–16.0

Forms a stable Cr₂O₃ oxide layer for superior oxidation resistance

Cobalt (Co)

8.5–10.0

Enhances strength and improves resistance to thermal fatigue

Molybdenum (Mo)

2.5–3.5

Increases creep resistance and strength under elevated temperatures

Titanium (Ti)

2.0–2.5

Forms strengthening phases (γ′, γ″) that enhance mechanical properties

Aluminum (Al)

1.0–2.0

Contributes to precipitation hardening via γ′ phase (Ni₃Al)

Iron (Fe)

≤1.0

Residual element

Carbon (C)

≤0.08

Carbide formation improves strength and wear resistance

Manganese (Mn)

≤0.5

Improves hot workability and reduces carbide formation

Silicon (Si)

≤0.5

Enhances oxidation resistance and high-temperature stability

Boron (B)

≤0.005

Strengthens grain boundaries and improves creep resistance

Zirconium (Zr)

≤0.05

Improves creep rupture strength and stability at high temperatures


Physical Properties

Property

Value (Typical)

Test Standard/Condition

Density

8.3 g/cm³

ASTM B311

Melting Range

1325–1375°C

ASTM E1268

Thermal Conductivity

13.2 W/m·K at 100°C

ASTM E1225

Electrical Resistivity

1.13 µΩ·m at 20°C

ASTM B193

Thermal Expansion

14.0 µm/m·°C (20–1000°C)

ASTM E228

Specific Heat Capacity

450 J/kg·K at 20°C

ASTM E1269

Elastic Modulus

210 GPa at 20°C

ASTM E111


Mechanical Properties (Solution Treated + Aged)

Property

Value (Typical)

Test Standard

Tensile Strength

1000–1200 MPa

ASTM E8/E8M

Yield Strength (0.2%)

800–950 MPa

ASTM E8/E8M

Elongation

≥20%

ASTM E8/E8M

Hardness

240–270 HB

ASTM E10

Creep Rupture Strength

210 MPa at 900°C (1000h)

ASTM E139

Fatigue Resistance

Excellent

ASTM E466


Key Characteristics of Rene 104

  • High-Temperature Strength and Fatigue Resistance Rene 104 retains exceptional tensile strength at elevated temperatures, with values exceeding 1000 MPa at temperatures up to 900°C, making it ideal for gas turbines and other high-temperature applications.

  • Precipitation Strengthening The alloy’s strength is primarily derived from the γ′ and γ″ phases, which provide high tensile and fatigue strength without compromising weldability.

  • Oxidation and Corrosion Resistance The chromium content enables the formation of a stable protective oxide layer, making Rene 104 highly resistant to oxidation in environments up to 1050°C.

  • Creep Resistance With a creep rupture strength of over 200 MPa at 900°C, Rene 104 is designed to withstand long-term thermal loads without significant deformation, ensuring the integrity of turbine blades and other components.

  • Good Weldability Rene 104’s chemistry allows for reliable weldability, with minimal hot cracking and good strength retention in the weld zone, making it suitable for both new parts and repair applications.


CNC Machining Challenges and Solutions for Rene 104

Machining Challenges

Tool Wear and Edge Chipping

  • The high hardness and presence of solid solution strengthening phases accelerate wear on carbide tools during machining.

Heat Generation

  • If not controlled, poor heat conductivity in Rene 104 leads to high cutting zone temperatures, which can cause tool degradation and dimensional distortion.

Work Hardening

  • The alloy exhibits significant work hardening during machining, which can lead to surface hardness increases of up to 30%.


Optimized Machining Strategies

Tool Selection

Parameter

Recommendation

Rationale

Tool Material

Carbide (K20–K30) or CBN inserts for finishing

High resistance to wear and high heat

Coating

AlTiN or TiSiN PVD (3–5 µm)

Reduces friction and heat buildup

Geometry

Positive rake angle (6–8°), sharp cutting edge (~0.05 mm)

Reduces cutting forces and work hardening

Cutting Parameters (ISO 3685 Compliant)

Operation

Speed (m/min)

Feed (mm/rev)

Depth of Cut (mm)

Coolant Pressure (bar)

Roughing

15–25

0.10–0.20

2.0–3.0

100–120

Finishing

30–40

0.05–0.08

0.3–0.8

120–150


Surface Treatment for Machined Rene 104 Parts

Hot Isostatic Pressing (HIP)

HIP improves part density and removes internal voids, enhancing fatigue strength by >25% for turbine components.

Heat Treatment

Heat Treatment includes solution treatment at ~1080°C followed by aging at 760°C to optimize the γ′ phase, increasing creep and fatigue resistance.

Superalloy Welding

Superalloy Welding ensures strong, crack-free welds with minimal strength loss across the heat-affected zone.

Thermal Barrier Coating (TBC)

TBC Coating reduces surface temperature by up to 250°C, significantly improving the durability of turbine blades and nozzles.

Electrical Discharge Machining (EDM)

EDM allows the creation of intricate features and cooling holes with tight tolerances, vital for high-performance components.

Deep Hole Drilling

Deep Hole Drilling ensures precise internal passages with L/D ratios >30:1 and a concentricity deviation <0.3 mm/m.

Material Testing and Analysis

Material Testing includes creep, tensile, and fatigue testing to confirm performance at elevated temperatures and microstructural analysis to verify γ′ phase distribution.


Industry Applications of Rene 104 Components

  • Aerospace Turbine Engines: Turbine blades, compressor discs, and seals exposed to cyclic thermal and mechanical stresses.

  • Power Generation: Gas turbine components such as blades, vanes, and nozzles operating in high-efficiency power plants.

  • Nuclear Reactors: Pressure vessels, reactor cores, and control rods exposed to thermal and radiation stresses.

  • Automotive Turbo Systems: Exhaust valves, turbocharger components, and heat-resistant engine parts.

  • Industrial Equipment: High-temperature furnace components, flanges, and valves requiring high creep resistance.


FAQs

  1. What machining challenges should be considered when processing Rene 104 for turbine components?

  2. How does the heat treatment process for Rene 104 impact its mechanical properties, especially its creep resistance?

  3. What surface treatment options are recommended for enhancing the fatigue strength of Rene 104 turbine blades?

  4. How does Rene 104’s machinability compare to other superalloys in high-temperature applications?

  5. What material testing requirements are for Rene 104 parts used in aerospace and power generation?

संबंधित ब्लॉग एक्सप्लोर करें