Monel R-405 is a free-machining version of the widely used Monel 400 nickel-copper alloy. Developed specifically for high-speed machining operations, Monel R-405 contains controlled sulfur additions to improve chip breaking and machinability without compromising the alloy’s excellent corrosion resistance.
Designed for high-volume production of threaded, precision, or valve components, Monel R-405 maintains good mechanical properties and seawater resistance while offering significantly better tool life and surface finish in CNC turning and automatic screw machine operations. It is commonly used in marine fittings, oil & gas tools, pump components, and electrical connectors.
Monel R-405 (UNS N04405 / ASTM B164) is a solid-solution nickel-copper alloy modified with sulfur to improve machinability. It is supplied in annealed or stress-relieved conditions to maximize its manufacturing performance.
| Element | Composition Range (wt.%) | Key Role | 
|---|---|---|
| Nickel (Ni) | ≥63.0 | Base element; corrosion resistance and toughness | 
| Copper (Cu) | 28.0–34.0 | Enhances resistance to acids and seawater | 
| Sulfur (S) | 0.025–0.060 | Improves machinability by promoting chip breakage | 
| Iron (Fe) | ≤2.5 | Strengthens the alloy | 
| Manganese (Mn) | ≤2.0 | Improves hot workability | 
| Silicon (Si) | ≤0.5 | Improves oxidation resistance | 
| Carbon (C) | ≤0.3 | Kept low to preserve weldability | 
| Property | Value (Typical) | Test Standard/Condition | 
|---|---|---|
| Density | 8.80 g/cm³ | ASTM B311 | 
| Melting Range | 1300–1350°C | ASTM E1268 | 
| Thermal Conductivity | 22.0 W/m·K at 100°C | ASTM E1225 | 
| Electrical Resistivity | 0.43 µΩ·m at 20°C | ASTM B193 | 
| Thermal Expansion | 13.9 µm/m·°C (20–300°C) | ASTM E228 | 
| Specific Heat Capacity | 427 J/kg·K at 20°C | ASTM E1269 | 
| Elastic Modulus | 179 GPa at 20°C | ASTM E111 | 
| Property | Value (Typical) | Test Standard | 
|---|---|---|
| Tensile Strength | 480–620 MPa | ASTM E8/E8M | 
| Yield Strength (0.2%) | 170–275 MPa | ASTM E8/E8M | 
| Elongation | ≥30% (25mm gauge) | ASTM E8/E8M | 
| Hardness | 120–180 HB | ASTM E10 | 
| Impact Toughness | Excellent at sub-zero temperatures | ASTM E23 | 
Enhanced Machinability: Sulfur content ensures shorter, curled chips that reduce tool loading and extend tool life by 25–40% over Monel 400.
Corrosion Resistance: Comparable to Monel 400 in seawater, brine, sulfuric acid, and hydrofluoric acid environments.
Non-Magnetic Stability: Remains non-magnetic in all processed forms, ideal for use near sensitive instrumentation.
High-Rate Machining Compatibility: Optimized for CNC lathes, screw machines, and high-speed precision turning of small components.
While more machinable than Monel 400, the material’s strength still causes moderate flank wear at high speeds without appropriate tooling.
Sulfur improves machinability but can slightly reduce weldability and surface polish capability if not properly managed during finishing.
At excessive feed rates, chip evacuation must be assisted with aggressive coolant delivery and sharp tool profiles.
| Parameter | Recommendation | Rationale | 
|---|---|---|
| Tool Material | Cobalt HSS or uncoated carbide | Maximizes edge retention for short runs | 
| Coating | TiN or TiCN (2–3 µm) | Reduces galling and improves chip release | 
| Geometry | 10–12° rake, sharp nose radius (0.4–0.8 mm) | Enhances surface finish and reduces work hardening | 
| Operation | Speed (m/min) | Feed (mm/rev) | DOC (mm) | Coolant Pressure (bar) | 
|---|---|---|---|---|
| Roughing | 30–50 | 0.20–0.30 | 2.0–3.0 | 80–100 | 
| Finishing | 50–80 | 0.05–0.10 | 0.5–1.0 | 100–120 | 
HIP is rarely required for Monel R-405 but can be applied for critical castings to enhance fatigue life and density.
Heat Treatment includes annealing at 850–900°C followed by controlled cooling to maintain machining-friendly microstructure.
Superalloy Welding is not recommended due to sulfur content; if needed, Monel 400 is preferred for weld-compatible assemblies.
TBC Coating is not common but may be used in high-temperature fittings requiring thermal shock protection.
EDM is well suited for precision slotting, threads, and intricate features in Monel R-405 without mechanical stress.
Deep Hole Drilling enables internal flow or alignment channels in compact oil & gas or marine parts.
Material Testing includes conductivity verification, microstructure analysis, sulfur distribution mapping, and mechanical property validation.
Shaft sleeves, valves, and seawater fittings.
Excellent resistance to flow-induced corrosion in brine and saltwater systems.
Threaded tool components, connectors, instrument housings.
Ideal for automated machining of large-volume precision parts in sour environments.
Pump shafts, fasteners, acid-resistant couplings.
Suitable for use in hydrofluoric acid and sulfur-rich processing lines.
Terminal pins, switch housings, and EMI-resistant mounts.
Non-magnetic and corrosion-resistant features support precision assemblies.
How does Monel R-405 improve machinability over Monel 400?
What CNC machining strategies work best for high-speed Monel R-405 parts?
Can Monel R-405 be welded or joined in high-integrity assemblies?
What surface finishes and tolerances are achievable with R-405?
How is sulfur controlled during material verification and QA?