Español

Stellite 6

A medium-hard cobalt-chromium-tungsten alloy offering excellent galling, corrosion, and wear resistance. Stellite 6 is well-suited for CNC-machined components in valve, pump, and thermal wear systems requiring long service life and dimensional integrity.

Introduction to Stellite 6

Stellite 6 is the most widely used cobalt-chromium alloy in the Stellite family due to its balanced combination of wear resistance, corrosion resistance, and moderate hardness. It performs excellently in metal-to-metal contact, low thermal conductivity environments, and corrosive fluids. Known for its galling resistance and stability at high temperatures, Stellite 6 is particularly well-suited for valve components, pump parts, and bearings that must endure continuous friction and corrosive attack.

This alloy is ideal for CNC-machined parts requiring long service life and dimensional precision in mechanical assemblies exposed to sliding wear and chemical exposure. Its adaptability, machinability (relative to harder Stellite grades), and performance consistency have made it a preferred material in aerospace, nuclear, petrochemical, and marine industries.


Chemical, Physical, and Mechanical Properties of Stellite 6

Stellite 6 (UNS R30006 / AMS 5387 / ISO 5832-4) is a cobalt-based alloy typically produced via casting, welding overlays, or powder metallurgy before CNC finishing.

Chemical Composition (Typical)

Element

Composition Range (wt.%)

Key Role

Cobalt (Co)

Balance (≥55.0)

Matrix phase providing hot hardness and corrosion resistance

Chromium (Cr)

27.0–32.0

Oxidation resistance and passivation in corrosive environments

Tungsten (W)

4.5–6.5

Carbide reinforcement for wear resistance

Carbon (C)

1.0–1.4

Moderate carbide content for anti-galling behavior

Nickel (Ni)

≤3.0

Increases toughness and ductility

Iron (Fe)

≤3.0

Residual alloying element

Silicon (Si)

≤1.2

Enhances fluidity and surface finish during casting

Manganese (Mn)

≤1.0

Improves hot workability


Physical Properties

Property

Value (Typical)

Test Standard/Condition

Density

8.65 g/cm³

ASTM B311

Melting Range

1240–1345°C

ASTM E1268

Thermal Conductivity

12.5 W/m·K at 100°C

ASTM E1225

Electrical Resistivity

0.96 µΩ·m at 20°C

ASTM B193

Thermal Expansion

12.7 µm/m·°C (20–400°C)

ASTM E228

Specific Heat Capacity

415 J/kg·K at 20°C

ASTM E1269

Elastic Modulus

210 GPa at 20°C

ASTM E111


Mechanical Properties (As-Cast or HIP + Heat Treated)

Property

Value (Typical)

Test Standard

Hardness

38–44 HRC (as-cast) / up to 46 HRC (HIP treated)

ASTM E18

Tensile Strength

800–1000 MPa

ASTM E8/E8M

Yield Strength (0.2%)

500–600 MPa

ASTM E8/E8M

Elongation

3–5%

ASTM E8/E8M

Wear Resistance Index

>2× 316 stainless steel

ASTM G65


Key Characteristics of Stellite 6

  • Outstanding Galling and Sliding Wear Resistance: Ideal for surfaces that experience continuous friction, even without lubrication.

  • Excellent Corrosion Resistance: Suitable for service in acidic, saline, and oxidizing media, including seawater and process chemicals.

  • Thermal Stability: Performs reliably at temperatures up to 800°C, retaining hardness and dimensional tolerance.

  • Machinability Advantage: Easier to CNC machine than harder grades like Stellite 3 or Stellite 12, while still offering excellent wear performance.


CNC Machining Challenges and Solutions for Stellite 6

Machining Challenges

Abrasive Carbide Phases

  • Tungsten carbides can dull tools quickly, especially under high-speed machining or improper tool coatings.

Built-Up Edge Formation

  • Flooding or material adhesion can occur without proper coolant and edge geometry, impacting tolerance and finish.

Moderate Work Hardening

  • Repeated tool passes may increase surface hardness, making finishing passes more difficult if not properly sequenced.


Optimized Machining Strategies

Tool Selection

Parameter

Recommendation

Rationale

Tool Material

Carbide (K30–K40), PVD-coated; CBN for finishing

Withstands abrasive carbides while providing edge retention

Coating

AlTiN or TiAlCrN (3–5 µm)

Reduces thermal wear and friction

Geometry

Neutral rake (0° to +5°), honed edge radius 0.02–0.05 mm

Minimizes cutting forces and tool chipping

Cutting Parameters (ISO 3685)

Operation

Speed (m/min)

Feed (mm/rev)

DOC (mm)

Coolant Pressure (bar)

Roughing

12–18

0.20–0.30

2.0–3.0

100–120

Finishing

22–30

0.05–0.10

0.5–1.0

120–150


Surface Treatment for Machined Stellite 6 Parts

Hot Isostatic Pressing (HIP)

HIP at 1150°C and 150 MPa eliminates porosity and enhances microstructural homogeneity, improving both fatigue and wear performance.

Heat Treatment

Heat Treatment can be used to relieve stress and fine-tune the distribution of carbides, ensuring long-term stability.

Superalloy Welding

Superalloy Welding using TIG or PTA overlays ensures wear zones remain robust after final CNC machining.

Thermal Barrier Coating (TBC)

TBC Coating increases performance in parts exposed to steam or gas erosion at elevated temperatures.

Electrical Discharge Machining (EDM)

EDM enables precise detail and tight tolerances in hardened parts, with Ra <0.6 µm.

Deep Hole Drilling

Deep Hole Drilling ensures accurate bore profiles in valve seats, nozzles, and wear-critical sleeves.

Material Testing and Analysis

Material Testing includes ASTM G65 wear tests, microstructure analysis, and hardness verification (ASTM E18).


Industry Applications of Stellite 6 Components

Valve Seats, Discs, and Guides

  • Reliable sealing and anti-galling performance in steam, chemical, and marine service valves.

Pump Bushings and Impellers

  • Resists cavitation and particulate erosion in slurry and process fluid environments.

Nuclear Power Systems

  • Control rod wear plates and valve internals operating under radiation and high pressure.

Marine and Oilfield Equipment

  • Shaft sleeves, gate valve seats, and wear-resistant trim exposed to saltwater and drilling fluids.


FAQs

  1. What are the optimal CNC cutting tools and speeds for machining Stellite 6?

  2. How does Stellite 6 compare to Stellite 3 and Stellite 12 in wear performance?

  3. Can Stellite 6 components be used in seawater or corrosive chemical environments?

  4. Is HIP recommended for cast Stellite 6 parts used in thermal cycling applications?

  5. What inspection and QA documentation is provided for CNC-machined Stellite 6 components?

Explorar blogs relacionados