Rene 80

Rene 80 is a nickel-based superalloy engineered for high-temperature applications requiring exceptional mechanical properties. With outstanding creep resistance, oxidation resistance, and weldability, Rene 80 is ideal for high-performance turbine blades and combustion components.

Introduction to Rene 80

Rene 80 is a high-performance nickel-based superalloy that is renowned for its outstanding resistance to oxidation, high-temperature strength, and mechanical properties in demanding environments. Commonly used in the aerospace, power generation, and industrial sectors, Rene 80 is designed to withstand extreme thermal and mechanical stresses. This alloy’s ability to maintain structural integrity under harsh conditions makes it ideal for components like turbine blades, combustion chambers, and exhaust systems.

To produce precision components from Rene 80, CNC machining services are indispensable. CNC machining ensures that Rene 80 parts meet the rigorous standards required in critical applications, including turbine engines and high-efficiency power systems.


Chemical, Physical, and Mechanical Properties of Rene 80

Rene 80 (UNS N07080 / W.Nr. 2.4962) is a nickel-chromium alloy engineered for high-temperature applications, providing exceptional resistance to oxidation and high mechanical strength under extreme conditions.

Chemical Composition (Typical)

Element

Composition Range (wt.%)

Key Role

Nickel (Ni)

Balance (~57.0)

Base matrix; provides high-temperature strength and oxidation resistance

Chromium (Cr)

14.0–16.0

Forms Cr₂O₃ oxide layer, offering superior oxidation resistance at high temperatures

Cobalt (Co)

9.0–11.0

Enhances thermal stability and strength in high-temperature environments

Molybdenum (Mo)

3.5–4.5

Increases creep resistance and overall high-temperature strength

Titanium (Ti)

3.0–4.0

Strengthens the alloy by forming the γ′ phase for better fatigue resistance

Aluminum (Al)

2.5–3.5

Contributes to the formation of the γ′ phase, improving strength and creep resistance

Iron (Fe)

≤1.0

Residual element

Carbon (C)

≤0.08

Forms carbides, improving high-temperature strength and wear resistance

Manganese (Mn)

≤1.0

Improves hot workability and reduces carbide formation

Silicon (Si)

≤0.5

Enhances oxidation resistance and high-temperature stability

Boron (B)

≤0.005

Improves grain boundary strength, enhancing creep resistance

Zirconium (Zr)

≤0.05

Increases creep rupture strength and enhances thermal stability


Physical Properties

Property

Value (Typical)

Test Standard/Condition

Density

8.7 g/cm³

ASTM B311

Melting Range

1350–1400°C

ASTM E1268

Thermal Conductivity

12.5 W/m·K at 100°C

ASTM E1225

Electrical Resistivity

1.20 µΩ·m at 20°C

ASTM B193

Thermal Expansion

15.0 µm/m·°C (20–1000°C)

ASTM E228

Specific Heat Capacity

460 J/kg·K at 20°C

ASTM E1269

Elastic Modulus

210 GPa at 20°C

ASTM E111


Mechanical Properties (Solution Treated + Aged)

Property

Value (Typical)

Test Standard

Tensile Strength

1100–1200 MPa

ASTM E8/E8M

Yield Strength (0.2%)

800–950 MPa

ASTM E8/E8M

Elongation

≥20%

ASTM E8/E8M

Hardness

250–280 HB

ASTM E10

Creep Rupture Strength

230 MPa at 900°C (1000h)

ASTM E139

Fatigue Resistance

Excellent

ASTM E466


Key Characteristics of Rene 80

  • High-Temperature Strength Rene 80 retains exceptional tensile strength exceeding 1100 MPa at temperatures up to 900°C, making it ideal for high-performance applications such as turbine blades and combustion chambers.

  • Precipitation Strengthening The alloy’s γ′ phase (Ni₃Ti) strengthens the material, providing outstanding creep resistance and fatigue strength, which is critical for parts exposed to long-term thermal cycling.

  • Oxidation and Corrosion Resistance The chromium and aluminum content in Rene 80 ensures the formation of a durable oxide layer, providing protection against oxidation and corrosion at temperatures up to 1050°C.

  • Creep Resistance Rene 80’s creep rupture strength of 230 MPa at 900°C ensures excellent long-term performance under mechanical stress and heat, making it ideal for turbine engines and industrial applications.

  • Weldability Rene 80 exhibits good weldability, allowing strong, crack-free welds to be made without significant loss of mechanical properties in the heat-affected zone, which is essential for both new manufacturing and repair of critical parts.


CNC Machining Challenges and Solutions for Rene 80

Machining Challenges

Tool Wear and Edge Chipping

  • The high hardness of Rene 80 leads to rapid tool wear, especially during aggressive cutting conditions, requiring specialized cutting tools such as carbide or CBN inserts.

Heat Generation

  • Rene 80’s low thermal conductivity causes significant heat buildup during machining, necessitating advanced cooling techniques to maintain dimensional stability and prevent tool failure.

Work Hardening

  • Rene 80 tends to work-harden during machining, which can result in surface hardness increases of 20–30%, requiring controlled cutting parameters to avoid tool deflection and dimensional inaccuracies.


Optimized Machining Strategies

Tool Selection

Parameter

Recommendation

Rationale

Tool Material

Carbide (K20–K30) or CBN inserts for finishing

Resists wear and maintains sharpness under high cutting temperatures

Coating

AlTiN or TiSiN PVD (3–5 µm)

Reduces friction and heat buildup

Geometry

Positive rake angle (6–8°), sharp cutting edge (~0.05 mm)

Minimizes cutting forces and prevents excessive tool wear

Cutting Parameters (ISO 3685 Compliant)

Operation

Speed (m/min)

Feed (mm/rev)

Depth of Cut (mm)

Coolant Pressure (bar)

Roughing

15–25

0.15–0.25

2.0–3.0

100–120

Finishing

30–40

0.05–0.10

0.3–0.8

120–150


Surface Treatment for Machined Rene 80 Parts

Hot Isostatic Pressing (HIP)

HIP reduces internal porosity and improves fatigue strength by more than 25%, essential for components exposed to high thermal and mechanical stresses.

Heat Treatment

Heat Treatment includes solution treatment at 1150°C followed by aging at 800°C to optimize γ′ phase formation, enhancing creep resistance and mechanical strength.

Superalloy Welding

Superalloy Welding provides crack-free, high-strength welds with minimal strength degradation in the heat-affected zone, ideal for repairs or joining critical turbine components.

Thermal Barrier Coating (TBC)

TBC Coating reduces surface temperatures by up to 250°C, extending the service life of high-temperature components like turbine blades and exhaust nozzles.

Electrical Discharge Machining (EDM)

EDM allows for the precise creation of intricate features such as cooling holes and microchannels, achieving tolerances as tight as ±0.005 mm.

Deep Hole Drilling

Deep Hole Drilling ensures precise internal passages for gas turbines, with L/D ratios up to 30:1 and concentricity deviations of less than 0.3 mm/m.

Material Testing and Analysis

Material Testing includes tensile, fatigue, and creep testing to confirm that components meet the high-temperature performance requirements of aerospace and industrial applications.


Industry Applications of Rene 80 Components


FAQs

  1. What are the machining challenges when processing Rene 80 for aerospace turbine applications?

  2. How does heat treatment improve the high-temperature performance of Rene 80 parts?

  3. What surface treatments are recommended for Rene 80 components operating in high-temperature environments?

  4. How does the workability of Rene 80 compare to other nickel-based superalloys?

  5. What material testing is necessary to ensure the reliability of Rene 80 in high-performance applications?