A cast nickel-based superalloy engineered with low carbon for improved weldability and casting reliability, offering high creep resistance, oxidation protection, and CNC machinability in turbine-grade applications.

Introduction to Inconel 738LC

Inconel 738LC is a low-carbon version of the cast nickel-based superalloy Inconel 738, designed to improve weldability, reduce hot cracking susceptibility, and enhance the structural integrity of cast components. It is engineered for service in high-temperature environments where mechanical strength, oxidation resistance, and creep performance are critical, particularly in aerospace turbines and industrial gas turbines.

Comprising nickel (~62%), chromium (16%), cobalt (8.5–9.5%), titanium (3.4–3.8%), and aluminum (3.2–3.7%), Inconel 738LC is strengthened primarily by the γ′ phase. Its optimized carbon content (0.02–0.06%) lowers the risk of microfissuring during welding and solidification, while preserving the high-temperature performance characteristics of the base alloy.


Chemical, Physical, and Mechanical Properties of Inconel 738LC

Inconel 738LC (UNS R30738 / ASTM A297, AMS 5391) is typically supplied in precision-cast, solution-treated, and age-hardened condition for gas turbine hot-section and aerospace structural applications.

Chemical Composition (Typical Cast Analysis)

Element

Composition Range (wt.%)

Key Role

Nickel (Ni)

~62.0

Base matrix for heat resistance and strength

Chromium (Cr)

15.5–16.5

Enhances oxidation and corrosion resistance

Cobalt (Co)

8.5–9.5

Increases fatigue strength and hot corrosion resistance

Tungsten (W)

2.6–3.3

Solid solution strengthening

Molybdenum (Mo)

1.5–2.1

Improves creep and rupture strength

Titanium (Ti)

3.4–3.8

Forms γ′ phase for age hardening

Aluminum (Al)

3.2–3.7

Contributes to γ′ precipitation

Carbon (C)

0.02–0.06

Reduced content improves weldability and casting reliability

Boron (B)

0.005–0.01

Enhances grain boundary ductility

Zirconium (Zr)

≤0.05

Grain boundary stabilization

Silicon (Si)

≤0.5

Oxidation resistance

Manganese (Mn)

≤0.5

Castability and cleanliness improvement


Physical Properties

Property

Value (Typical)

Test Standard/Condition

Density

8.15 g/cm³

ASTM B311

Melting Range

1260–1330°C

ASTM E1268

Thermal Conductivity

11.1 W/m·K at 100°C

ASTM E1225

Electrical Resistivity

1.28 µΩ·m at 20°C

ASTM B193

Thermal Expansion

13.3 µm/m·°C (20–1000°C)

ASTM E228

Specific Heat Capacity

450 J/kg·K at 20°C

ASTM E1269

Elastic Modulus

188 GPa at 20°C

ASTM E111


Mechanical Properties (Cast + Aged Condition)

Property

Value (Typical)

Test Standard

Tensile Strength

980–1100 MPa

ASTM E8/E8M

Yield Strength (0.2%)

680–800 MPa

ASTM E8/E8M

Elongation

≥4–8% (25mm gauge)

ASTM E8/E8M

Hardness

320–390 HB

ASTM E10

Creep Rupture Strength

≥135 MPa @ 870°C, 1000h

ASTM E139


Key Characteristics of Inconel 738LC

  • Low Carbon Content: Reduces hot cracking during welding and casting, enhancing reliability in structural turbine parts.

  • High Gamma Prime Content: Strengthened primarily by γ′ precipitates, it delivers excellent creep and fatigue resistance at elevated temperatures.

  • Dimensional and Structural Stability: Maintains geometry and load-bearing performance up to 980°C under thermal cycling.

  • CNC Machinability: Compatible with high-performance cutting tools, Inconel 738LC can be CNC machined to tight tolerances (±0.02 mm) with surface finishes of Ra ≤ 0.8 µm.


CNC Machining Challenges and Solutions for Inconel 738LC

Machining Challenges

High Surface Hardness

  • Brinell hardness near 390 HB leads to rapid wear on cutting edges, requiring optimized tool materials and geometries.

Poor Heat Dissipation

  • Low thermal conductivity accumulates heat at the tool–chip interface, causing crater wear and tool failure without adequate cooling.

Abrasive Microstructure

  • γ′ and carbide phases promote notching and galling during interrupted or high-feed machining operations.


Optimized Machining Strategies

Tool Selection

Parameter

Recommendation

Rationale

Tool Material

Ceramic (SiAlON) or coated carbide

Maintains cutting edge under thermal load

Coating

TiAlN, AlCrN (3–6 µm PVD)

Reduces heat diffusion and tool oxidation

Geometry

Positive rake (10–12°), edge-honed inserts

Minimizes cutting resistance and chipping

Cutting Parameters (ISO 3685)

Operation

Speed (m/min)

Feed (mm/rev)

DOC (mm)

Coolant Pressure (bar)

Roughing

15–25

0.20–0.30

2.0–3.0

80–100

Finishing

30–45

0.05–0.10

0.3–0.8

100–150


Surface Treatment for Machined Inconel 738LC Parts

Hot Isostatic Pressing (HIP)

HIP eliminates porosity and strengthens grain structure, improving fatigue life and creep resistance by up to 25%.

Heat Treatment

Heat Treatment uses solution annealing at 1120–1170°C and aging at 845°C to fully precipitate γ′, enhancing high-temperature strength.

Superalloy Welding

Superalloy Welding is feasible with reduced cracking risk due to low carbon. Preheat and post-weld heat treatment further stabilize the microstructure.

Thermal Barrier Coating (TBC)

TBC Coating applies 125–250 µm of YSZ ceramics via APS or EB-PVD to reduce thermal fatigue and oxidation in turbine blades.

Electrical Discharge Machining (EDM)

EDM achieves intricate geometries, cooling slots, and sharp features with ±0.01 mm precision post-casting.

Deep Hole Drilling

Deep Hole Drilling enables high L/D ratio cooling bores and oil channels essential in turbine airfoils and rotor structures.

Material Testing and Analysis

Material Testing verifies alloy integrity through tensile, creep, hardness, and microstructure analysis per ASTM E112 and AMS 5391.


Industry Applications of Inconel 738LC Components

Aerospace Turbines

  • Guide vanes, shroud segments, and nozzle components.

  • Reliable under high rotational stress and extreme thermal cycling.

Power Generation

  • Hot section castings in gas turbines including combustion chambers and seals.

  • Maintains shape and strength during extended base-load operation at 950°C+.

Marine & Energy

  • High-temperature pump housings, exhaust valves, and turbine discs.

  • Resistant to corrosion and thermal distortion in harsh offshore environments.

Defense Propulsion Systems

  • Jet engine hot parts and afterburner elements.

  • Delivers consistent performance through rapid heating and cooling cycles.


FAQs

  1. How does Inconel 738LC improve casting and welding reliability compared to Inconel 738?

  2. What CNC machining practices are best for maintaining tool life with Inconel 738LC?

  3. Is HIP necessary for high-cycle fatigue applications in Inconel 738LC?

  4. Can Neway provide integrated services from casting to TBC for Inconel 738LC parts?

  5. What quality standards are used to inspect and validate Inconel 738LC turbine components?

Explorar blogs relacionados