English

Stellite F

Stellite F is a high-performance cobalt-based alloy ideal for CNC-machined parts subjected to galling, thermal fatigue, and corrosion in high-speed, high-temperature environments. It offers a unique balance of wear resistance, structural integrity, and processability for critical industrial components.

Introduction to Stellite F

Stellite F is a cast cobalt-based alloy specifically designed for high-strength, high-temperature applications requiring galling resistance, thermal fatigue stability, and corrosion performance. It is commonly used for high-speed components like valve rotors, seals, and steam turbine parts where exposure to thermal cycling, frictional wear, and aggressive process media is continuous and severe.

Stellite F exhibits excellent workability and mechanical uniformity as a cast-wrought hybrid material, making it ideal for post-processing using advanced CNC machining. It retains hardness up to 1000°C and performs exceptionally well under metal-to-metal sliding contact, particularly in rotating or sealing applications.


Chemical, Physical, and Mechanical Properties of Stellite F

Stellite F (UNS R30665) is characterized by a moderate carbon content with a well-balanced chromium and tungsten matrix, offering high resistance to galling, oxidation, and impact under heat.

Chemical Composition (Typical)

Element

Composition Range (wt.%)

Key Role

Cobalt (Co)

Balance (≥50.0)

Matrix for high-temperature strength and corrosion resistance

Chromium (Cr)

25.0–28.0

Enhances oxidation resistance and forms protective surface scales

Tungsten (W)

4.5–6.5

Forms hard carbide phases for wear protection

Carbon (C)

0.9–1.2

Controls carbide volume for strength and hardness

Iron (Fe)

≤3.0

Residual element

Nickel (Ni)

≤2.5

Improves ductility and casting properties

Silicon (Si)

≤1.2

Aids in oxidation resistance and casting flow

Manganese (Mn)

≤1.0

Improves hot ductility and microstructure integrity


Physical Properties

Property

Value (Typical)

Test Standard/Condition

Density

8.7 g/cm³

ASTM B311

Melting Range

1300–1385°C

ASTM E1268

Thermal Conductivity

13.0 W/m·K at 100°C

ASTM E1225

Electrical Resistivity

0.96 µΩ·m at 20°C

ASTM B193

Thermal Expansion

12.8 µm/m·°C (20–400°C)

ASTM E228

Specific Heat Capacity

420 J/kg·K at 20°C

ASTM E1269

Elastic Modulus

210 GPa at 20°C

ASTM E111


Mechanical Properties (As-Cast or HIP-Treated)

Property

Value (Typical)

Test Standard

Hardness

40–47 HRC (as-cast) / up to 50 HRC (HIP)

ASTM E18

Tensile Strength

980–1100 MPa

ASTM E8/E8M

Yield Strength (0.2%)

520–640 MPa

ASTM E8/E8M

Elongation

3.0–4.0%

ASTM E8/E8M

Galling Resistance

Excellent

ASTM G98

Operating Temperature

Up to 1000°C

N/A


Key Characteristics of Stellite F

  • High Galling and Wear Resistance: Designed for sliding contact under pressure, Stellite F resists adhesion and material transfer in dry and lubricated conditions.

  • Thermal Fatigue Strength: Performs well under repeated heating and cooling cycles with minimal dimensional drift or surface damage.

  • Corrosion and Oxidation Resistance: Effective in resisting acidic and oxidizing process environments, including high-pressure steam and combustion gases.

  • Impact and Cavitation Resistance: Withstands cyclic stress and cavitation forces in high-speed rotating systems such as pumps and turbines.


CNC Machining Challenges and Solutions for Stellite F

Machining Challenges

Galling During Tool Engagement

  • Due to its adhesive resistance properties, cutting tools can experience rubbing instead of shearing, leading to chatter or built-up edge formation.

Low Thermal Conductivity

  • Heat generated during cutting accumulates at the tool tip, increasing the risk of microcracks or thermal degradation of carbide inserts.

Abrasive Carbide Network

  • Moderate carbide content wears tooling aggressively, particularly during roughing or interrupted cuts.


Optimized Machining Strategies

Tool Selection

Parameter

Recommendation

Rationale

Tool Material

K30-grade carbide or CBN inserts

Offers balance between hardness and fracture toughness

Coating

AlCrN or TiSiN (PVD 3–5 µm)

Provides thermal protection and reduces friction

Geometry

Neutral rake with 0.05 mm edge hone

Supports cutting integrity and mitigates edge chipping

Cutting Parameters (ISO 3685 Compliant)

Operation

Speed (m/min)

Feed (mm/rev)

Depth of Cut (mm)

Coolant Pressure (bar)

Roughing

10–14

0.20–0.30

1.5–2.0

100–120

Finishing

18–22

0.05–0.10

0.5–1.0

120–150


Surface Treatment for Machined Stellite F Parts

Hot Isostatic Pressing (HIP)

HIP enhances fatigue and creep resistance while eliminating internal porosity in as-cast parts.

Heat Treatment

Heat Treatment stabilizes the carbide structure, relieves stress, and improves hardness uniformity across machined zones.

Superalloy Welding

Superalloy Welding using filler materials with matching chemistry ensures joint integrity in high-wear or corrosive systems.

Thermal Barrier Coating (TBC)

TBC Coating provides added insulation for surfaces operating in hot gas flows above 950°C.

Electrical Discharge Machining (EDM)

EDM is ideal for achieving ±0.01 mm tolerance in valve features, orifices, and complex contours.

Deep Hole Drilling

Deep Hole Drilling enables manufacturing of deep-seated bores or cooling channels without compromising structural stability.

Material Testing and Analysis

Material Testing includes hardness testing, microstructure validation, galling resistance trials, and non-destructive testing (UT, PT).


Industry Applications of Stellite F Components

Turbine and Steam Plant Hardware

  • Valve rotors, deflector rings, and seat faces operating in extreme temperatures and rotational speeds.

High-Pressure Sealing Components

  • Sliding seals, pump sleeves, and rotary joints in chemical, power generation, and aerospace sectors.

Marine & Desalination Equipment

  • Pump housings, shaft sleeves, and wear plates exposed to brine, cavitation, and thermal fluctuation.

Oil & Gas

  • Valve internals, guide rings, and cutting tools subject to sand erosion, chemical attack, and pressure cycling.


Explore Related Blogs

Copyright © 2026 Machining Precision Works Ltd.All Rights Reserved.