Stellite 6K

Wrought cobalt-based alloy with exceptional galling resistance and mechanical toughness. Stellite 6K is ideal for CNC-machined components in valves, bearings, and wear surfaces requiring dry sliding resistance and long-term durability under harsh conditions.

Introduction to Stellite 6K

Stellite 6K is a wrought cobalt-chromium alloy specifically engineered for enhanced toughness, galling resistance, and wear performance in metal-to-metal contact applications. It shares a similar chemical composition with Stellite 6B but features higher ductility and improved machinability due to its fine-grained wrought microstructure. The "K" variant is optimized for sliding wear under pressure, impact, and thermal stress applications.

Stellite 6K is ideal for CNC-machined components where both dimensional accuracy and resistance to seizing, scuffing, and erosion are critical. Common applications include bushings, bearings, pump sleeves, and valve stems used in aerospace, marine, energy, and oil & gas industries.


Chemical, Physical, and Mechanical Properties of Stellite 6K

Stellite 6K (UNS R30016 / ASTM F90, AMS 5894 derivative) is a solid-solution strengthened cobalt alloy manufactured by hot working, forging, or rolling to achieve a homogeneous, dense structure with superior mechanical integrity.

Chemical Composition (Typical)

Element

Composition Range (wt.%)

Key Role

Cobalt (Co)

Balance (≥58.0)

Base matrix for corrosion and high-temperature strength

Chromium (Cr)

28.0–32.0

Provides oxidation and corrosion resistance

Tungsten (W)

4.5–6.5

Forms carbides to improve wear resistance

Carbon (C)

0.9–1.4

Controls carbide formation to resist galling

Nickel (Ni)

≤3.0

Enhances toughness and ductility

Iron (Fe)

≤3.0

Residual element

Manganese (Mn)

≤1.0

Supports hot workability

Silicon (Si)

≤1.2

Improves casting fluidity and surface finish


Physical Properties

Property

Value (Typical)

Test Standard/Condition

Density

8.42 g/cm³

ASTM B311

Melting Range

1320–1395°C

ASTM E1268

Thermal Conductivity

13.0 W/m·K at 100°C

ASTM E1225

Electrical Resistivity

0.96 µΩ·m at 20°C

ASTM B193

Thermal Expansion

13.2 µm/m·°C (20–400°C)

ASTM E228

Specific Heat Capacity

420 J/kg·K at 20°C

ASTM E1269

Elastic Modulus

205 GPa at 20°C

ASTM E111


Mechanical Properties (Wrought Condition)

Property

Value (Typical)

Test Standard

Hardness

33–43 HRC (annealed) / up to 45 HRC (aged)

ASTM E18

Tensile Strength

1050–1200 MPa

ASTM E8/E8M

Yield Strength (0.2%)

550–700 MPa

ASTM E8/E8M

Elongation

10–20%

ASTM E8/E8M

Galling Resistance

Excellent, even against itself

ASTM G98

Wear Resistance Index

>2.5× 316 stainless steel

ASTM G65


Key Characteristics of Stellite 6K

  • Superior Galling Resistance: Outstanding performance under metal-to-metal contact, even in dry sliding conditions.

  • High Toughness and Ductility: More forgiving in impact-prone environments than cast Stellite grades, reducing the risk of cracking or edge chipping.

  • Thermal and Corrosive Stability: Withstands service temperatures up to 850°C and resists pitting and oxidation in chlorides and acids.

  • Improved Machinability: Compared to cast Stellite 6, the wrought 6K form provides better dimensional control during CNC machining.


CNC Machining Challenges and Solutions for Stellite 6K

Machining Challenges

Abrasive Carbide Phases

  • The tungsten-rich carbides increase tool wear, particularly during prolonged roughing passes.

Heat Buildup at the Tool-Work Interface

  • Low thermal conductivity traps heat in the cutting zone, degrading tool coatings and accuracy.

Work Hardening

  • Repeated tool passes can raise surface hardness, requiring careful pass planning and tool monitoring.


Optimized Machining Strategies

Tool Selection

Parameter

Recommendation

Rationale

Tool Material

PVD-coated carbide (K30–K40); CBN for tight-finish tolerances

Handles abrasive wear while maintaining edge strength

Coating

AlTiN or TiAlCrN (3–5 µm)

Lowers cutting zone temperature and prolongs tool life

Geometry

Neutral rake (0°), honed cutting edge 0.03 mm

Enhances cutting edge durability and prevents chip adhesion

Cutting Parameters (ISO 3685)

Operation

Speed (m/min)

Feed (mm/rev)

DOC (mm)

Coolant Pressure (bar)

Roughing

10–18

0.20–0.30

2.0–3.0

100–120

Finishing

20–28

0.05–0.10

0.5–1.0

120–150


Surface Treatment for Machined Stellite 6K Parts

Hot Isostatic Pressing (HIP)

HIP is generally unnecessary for wrought Stellite 6K but may be used on powder metallurgy or additively manufactured forms to enhance fatigue life.

Heat Treatment

Heat Treatment post-machining can optimize carbide distribution and reduce residual stress from forming or CNC cutting.

Superalloy Welding

Superalloy Welding using low-dilution PTA or TIG welding techniques with matching filler helps retain wear and galling resistance across joints.

Thermal Barrier Coating (TBC)

TBC Coating protects against hot gas erosion and enhances high-temperature durability in rotating and reciprocating parts.

Electrical Discharge Machining (EDM)

EDM ensures precise finishing of tight-tolerance parts with Ra <0.5 µm in hardened or complex geometries.

Deep Hole Drilling

Deep Hole Drilling is suitable for creating wear-resistant bushings and flow-control components with aspect ratios >20:1.

Material Testing and Analysis

Material Testing includes tensile strength, microhardness profiling, metallographic examination, and ASTM G98 galling evaluation.


Industry Applications of Stellite 6K Components

Industrial Valve Systems

  • Valve stems, guides, and plug components that must resist galling under pressure and temperature extremes.

Aerospace Bearings and Linkages

  • Precision bushings and control system components operating in dry or lubricated sliding contact.

Oil & Gas Equipment

  • Drill head stabilizers, pump sleeves, and rotating seals subjected to slurry abrasion and corrosive fluids.

Power Generation and Turbomachinery

  • Hot section wear pads and sealing surfaces exposed to high thermal and cyclic loading.