Rene 80 is a high-performance nickel-based superalloy that is renowned for its outstanding resistance to oxidation, high-temperature strength, and mechanical properties in demanding environments. Commonly used in the aerospace, power generation, and industrial sectors, Rene 80 is designed to withstand extreme thermal and mechanical stresses. This alloy’s ability to maintain structural integrity under harsh conditions makes it ideal for components like turbine blades, combustion chambers, and exhaust systems.
To produce precision components from Rene 80, CNC machining services are indispensable. CNC machining ensures that Rene 80 parts meet the rigorous standards required in critical applications, including turbine engines and high-efficiency power systems.
Rene 80 (UNS N07080 / W.Nr. 2.4962) is a nickel-chromium alloy engineered for high-temperature applications, providing exceptional resistance to oxidation and high mechanical strength under extreme conditions.
Element | Composition Range (wt.%) | Key Role |
|---|---|---|
Nickel (Ni) | Balance (~57.0) | Base matrix; provides high-temperature strength and oxidation resistance |
Chromium (Cr) | 14.0–16.0 | Forms Cr₂O₃ oxide layer, offering superior oxidation resistance at high temperatures |
Cobalt (Co) | 9.0–11.0 | Enhances thermal stability and strength in high-temperature environments |
Molybdenum (Mo) | 3.5–4.5 | Increases creep resistance and overall high-temperature strength |
Titanium (Ti) | 3.0–4.0 | Strengthens the alloy by forming the γ′ phase for better fatigue resistance |
Aluminum (Al) | 2.5–3.5 | Contributes to the formation of the γ′ phase, improving strength and creep resistance |
Iron (Fe) | ≤1.0 | Residual element |
Carbon (C) | ≤0.08 | Forms carbides, improving high-temperature strength and wear resistance |
Manganese (Mn) | ≤1.0 | Improves hot workability and reduces carbide formation |
Silicon (Si) | ≤0.5 | Enhances oxidation resistance and high-temperature stability |
Boron (B) | ≤0.005 | Improves grain boundary strength, enhancing creep resistance |
Zirconium (Zr) | ≤0.05 | Increases creep rupture strength and enhances thermal stability |
Property | Value (Typical) | Test Standard/Condition |
|---|---|---|
Density | 8.7 g/cm³ | ASTM B311 |
Melting Range | 1350–1400°C | ASTM E1268 |
Thermal Conductivity | 12.5 W/m·K at 100°C | ASTM E1225 |
Electrical Resistivity | 1.20 µΩ·m at 20°C | ASTM B193 |
Thermal Expansion | 15.0 µm/m·°C (20–1000°C) | ASTM E228 |
Specific Heat Capacity | 460 J/kg·K at 20°C | ASTM E1269 |
Elastic Modulus | 210 GPa at 20°C | ASTM E111 |
Property | Value (Typical) | Test Standard |
|---|---|---|
Tensile Strength | 1100–1200 MPa | ASTM E8/E8M |
Yield Strength (0.2%) | 800–950 MPa | ASTM E8/E8M |
Elongation | ≥20% | ASTM E8/E8M |
Hardness | 250–280 HB | ASTM E10 |
Creep Rupture Strength | 230 MPa at 900°C (1000h) | ASTM E139 |
Fatigue Resistance | Excellent | ASTM E466 |
High-Temperature Strength Rene 80 retains exceptional tensile strength exceeding 1100 MPa at temperatures up to 900°C, making it ideal for high-performance applications such as turbine blades and combustion chambers.
Precipitation Strengthening The alloy’s γ′ phase (Ni₃Ti) strengthens the material, providing outstanding creep resistance and fatigue strength, which is critical for parts exposed to long-term thermal cycling.
Oxidation and Corrosion Resistance The chromium and aluminum content in Rene 80 ensures the formation of a durable oxide layer, providing protection against oxidation and corrosion at temperatures up to 1050°C.
Creep Resistance Rene 80’s creep rupture strength of 230 MPa at 900°C ensures excellent long-term performance under mechanical stress and heat, making it ideal for turbine engines and industrial applications.
Weldability Rene 80 exhibits good weldability, allowing strong, crack-free welds to be made without significant loss of mechanical properties in the heat-affected zone, which is essential for both new manufacturing and repair of critical parts.
The high hardness of Rene 80 leads to rapid tool wear, especially during aggressive cutting conditions, requiring specialized cutting tools such as carbide or CBN inserts.
Rene 80’s low thermal conductivity causes significant heat buildup during machining, necessitating advanced cooling techniques to maintain dimensional stability and prevent tool failure.
Rene 80 tends to work-harden during machining, which can result in surface hardness increases of 20–30%, requiring controlled cutting parameters to avoid tool deflection and dimensional inaccuracies.
Parameter | Recommendation | Rationale |
|---|---|---|
Tool Material | Carbide (K20–K30) or CBN inserts for finishing | Resists wear and maintains sharpness under high cutting temperatures |
Coating | AlTiN or TiSiN PVD (3–5 µm) | Reduces friction and heat buildup |
Geometry | Positive rake angle (6–8°), sharp cutting edge (~0.05 mm) | Minimizes cutting forces and prevents excessive tool wear |
Operation | Speed (m/min) | Feed (mm/rev) | Depth of Cut (mm) | Coolant Pressure (bar) |
|---|---|---|---|---|
Roughing | 15–25 | 0.15–0.25 | 2.0–3.0 | 100–120 |
Finishing | 30–40 | 0.05–0.10 | 0.3–0.8 | 120–150 |
HIP reduces internal porosity and improves fatigue strength by more than 25%, essential for components exposed to high thermal and mechanical stresses.
Heat Treatment includes solution treatment at 1150°C followed by aging at 800°C to optimize γ′ phase formation, enhancing creep resistance and mechanical strength.
Superalloy Welding provides crack-free, high-strength welds with minimal strength degradation in the heat-affected zone, ideal for repairs or joining critical turbine components.
TBC Coating reduces surface temperatures by up to 250°C, extending the service life of high-temperature components like turbine blades and exhaust nozzles.
EDM allows for the precise creation of intricate features such as cooling holes and microchannels, achieving tolerances as tight as ±0.005 mm.
Deep Hole Drilling ensures precise internal passages for gas turbines, with L/D ratios up to 30:1 and concentricity deviations of less than 0.3 mm/m.
Material Testing includes tensile, fatigue, and creep testing to confirm that components meet the high-temperature performance requirements of aerospace and industrial applications.
Aerospace Turbine Engines: Turbine blades, vanes, and nozzles exposed to extreme thermal and mechanical stresses.
Power Generation: Gas turbine blades, vanes, and exhaust nozzles for high-efficiency turbines.
Nuclear Reactors: Reactor core components, pressure vessels, and heat exchangers exposed to high radiation and thermal stresses.
Automotive Turbo Systems: Turbochargers, exhaust valves, and heat shields for high-performance vehicles.
Industrial Heat Treatment Equipment: Furnace components, seals, and fixtures exposed to high temperatures in industrial applications.