Rene 77 is a high-performance nickel-based superalloy that maintains exceptional strength and stability in high-temperature environments. Known for its excellent creep resistance, oxidation resistance, and ability to perform in extreme thermal and mechanical stresses, Rene 77 is widely used in the aerospace, energy, and industrial sectors. This alloy is particularly useful for components that must endure long-term exposure to high temperatures, such as turbine blades, combustion chambers, and exhaust systems.
To achieve the tight tolerances and complex geometries required for such applications, CNC machining services are crucial. CNC machining enables the precise fabrication of critical components like turbine blades, seals, and other parts that demand the high level of performance and reliability offered by Rene 77.
Rene 77 (UNS N07077 / W.Nr. 2.4966) is a nickel-based superalloy formulated for use in the most demanding applications, particularly in environments with high thermal and mechanical stresses.
Element | Composition Range (wt.%) | Key Role |
|---|---|---|
Nickel (Ni) | Balance (~56.0) | Base matrix; provides oxidation resistance and high-temperature strength |
Chromium (Cr) | 13.0–15.0 | Forms Cr₂O₃ oxide layer, providing superior oxidation resistance at high temperatures |
Cobalt (Co) | 9.5–11.5 | Increases high-temperature strength and resistance to thermal fatigue |
Molybdenum (Mo) | 3.0–4.0 | Strengthens the alloy and increases resistance to creep |
Titanium (Ti) | 3.0–4.5 | Forms γ′ phase for precipitation strengthening, increasing mechanical properties |
Aluminum (Al) | 2.5–3.5 | Contributes to the formation of the γ′ phase, enhancing strength and creep resistance |
Iron (Fe) | ≤1.0 | Residual element |
Carbon (C) | ≤0.08 | Forms carbides to improve high-temperature strength and wear resistance |
Manganese (Mn) | ≤1.0 | Enhances hot workability and reduces carbide formation |
Silicon (Si) | ≤0.5 | Improves oxidation resistance and high-temperature stability |
Boron (B) | ≤0.005 | Strengthens grain boundaries, improving creep resistance |
Zirconium (Zr) | ≤0.05 | Increases creep rupture strength and thermal stability at high temperatures |
Property | Value (Typical) | Test Standard/Condition |
|---|---|---|
Density | 8.6 g/cm³ | ASTM B311 |
Melting Range | 1340–1380°C | ASTM E1268 |
Thermal Conductivity | 13.2 W/m·K at 100°C | ASTM E1225 |
Electrical Resistivity | 1.15 µΩ·m at 20°C | ASTM B193 |
Thermal Expansion | 14.7 µm/m·°C (20–1000°C) | ASTM E228 |
Specific Heat Capacity | 460 J/kg·K at 20°C | ASTM E1269 |
Elastic Modulus | 215 GPa at 20°C | ASTM E111 |
Property | Value (Typical) | Test Standard |
|---|---|---|
Tensile Strength | 1150–1250 MPa | ASTM E8/E8M |
Yield Strength (0.2%) | 800–950 MPa | ASTM E8/E8M |
Elongation | ≥20% | ASTM E8/E8M |
Hardness | 240–280 HB | ASTM E10 |
Creep Rupture Strength | 230 MPa at 900°C (1000h) | ASTM E139 |
Fatigue Resistance | Excellent | ASTM E466 |
High-Temperature Strength Rene 77 maintains a tensile strength exceeding 1150 MPa at temperatures up to 900°C, making it ideal for turbine blades and other high-performance aerospace components.
Precipitation Strengthening The γ′ phase (Ni₃Ti) is a key contributor to Rene 77’s excellent strength and fatigue resistance, making it well-suited for long-term use in thermal cycling environments.
Oxidation and Corrosion Resistance The alloy’s chromium and aluminum content helps form a stable oxide layer that provides superior resistance to oxidation and corrosion, even at elevated temperatures up to 1050°C.
Creep Resistance Rene 77 exhibits a creep rupture strength of over 230 MPa at 900°C, ensuring long-term stability in high-stress, high-temperature applications such as turbine engines.
Weldability Rene 77 has excellent weldability, allowing for strong, crack-free welds in high-performance turbine and engine components with minimal degradation of mechanical properties in the heat-affected zone.
The high hardness and solid solution strengthening phases in Rene 77 increase the tool wear rate, particularly when using carbide tools under aggressive machining conditions.
Due to its low thermal conductivity, Rene 77 generates high cutting temperatures, requiring effective cooling methods to prevent tool damage and maintain dimensional accuracy.
Rene 77 exhibits significant work hardening during machining, which can cause an increase in surface hardness by 20–30%, potentially leading to tool wear and poor surface finish if not carefully controlled.
Parameter | Recommendation | Rationale |
|---|---|---|
Tool Material | Carbide (K20–K30) or CBN inserts for finishing | Excellent wear resistance under high cutting temperatures |
Coating | AlTiN or TiSiN PVD (3–5 µm) | Reduces friction and heat buildup |
Geometry | Positive rake angle (6–8°), sharp cutting edge (~0.05 mm) | Minimizes cutting forces and prevents excessive tool wear |
Operation | Speed (m/min) | Feed (mm/rev) | Depth of Cut (mm) | Coolant Pressure (bar) |
|---|---|---|---|---|
Roughing | 15–25 | 0.15–0.25 | 2.0–3.0 | 100–120 |
Finishing | 30–40 | 0.05–0.10 | 0.3–0.8 | 120–150 |
HIP reduces internal porosity, improving the fatigue strength of Rene 77 components by over 25%, essential for high-stress applications in aerospace turbines.
Heat Treatment includes solution treatment at 1150°C followed by aging at 800°C to optimize the formation of the γ′ phase, enhancing creep resistance and tensile strength.
Superalloy Welding enables crack-free, high-strength welds with minimal loss of mechanical properties in the heat-affected zone, ideal for repairing or joining critical turbine components.
TBC Coating extends the service life of turbine blades by reducing surface operating temperatures by up to 200°C, improving performance in high-temperature environments.
EDM allows for precise machining of internal cooling passages and other microfeatures, achieving tolerances as tight as ±0.005 mm without thermal distortion.
Deep Hole Drilling ensures high-accuracy internal passages needed for gas turbines, with L/D ratios up to 30:1 and concentricity deviations of less than 0.3 mm/m.
Material Testing includes tensile, creep, and fatigue testing to ensure that Rene 77 components meet the rigorous mechanical and thermal performance requirements for critical aerospace applications.
Aerospace Turbine Engines: Turbine blades, vanes, and discs subjected to high thermal and mechanical stresses.
Power Generation: Gas turbine components such as blades, vanes, and exhaust nozzles for high-efficiency turbines.
Nuclear Reactors: Reactor core components, pressure vessels, and control rods exposed to high radiation and thermal conditions.
Automotive Turbo Systems: Turbocharger components, exhaust valves, and heat shields for high-performance vehicles.
Industrial Heat Treatment Equipment: Furnace parts, seals, and fixtures exposed to high temperatures in industrial applications.