Nimonic PE11 is a high-performance nickel-based superalloy engineered for exceptional strength and oxidation resistance at elevated temperatures. Designed for use in applications where resistance to both thermal fatigue and creep is essential, Nimonic PE11 is commonly used in critical aerospace, power generation, and nuclear applications. The alloy’s solid solution strengthening mechanism, combined with a high chromium content, allows it to maintain its structural integrity under extreme mechanical and thermal stress.
To meet the strict dimensional tolerances required for these high-stress applications, Nimonic PE11 is often processed through CNC machining services. CNC machining enables precise, repeatable manufacturing of complex geometries, ensuring reliable performance in extreme environments.
Nimonic PE11 (UNS N07011 / W.Nr. 2.4952) is a high-strength, heat-resistant alloy primarily used in turbine blades, nozzle guide vanes, and other aerospace and industrial gas turbine components.
Element | Composition Range (wt.%) | Key Role |
|---|---|---|
Nickel (Ni) | Balance (≥50.0) | The base matrix; provides corrosion resistance and thermal stability |
Chromium (Cr) | 15.0–17.0 | Forms Cr₂O₃ oxide layer to resist high-temperature oxidation |
Cobalt (Co) | 10.0–12.0 | Strengthens the matrix and improves thermal fatigue resistance |
Molybdenum (Mo) | 2.0–3.0 | Enhances creep resistance and solid solution strengthening |
Titanium (Ti) | 3.0–4.0 | Contributes to γ′ phase for precipitation hardening |
Aluminum (Al) | 2.0–3.0 | Precipitation strengthening via Ni₃Al phase |
Iron (Fe) | ≤2.0 | Residual element |
Carbon (C) | ≤0.08 | Carbide formation improves creep and fatigue strength |
Manganese (Mn) | ≤1.0 | Enhances hot workability |
Silicon (Si) | ≤0.5 | Improves oxidation resistance |
Boron (B) | ≤0.01 | Grain boundary strengthening |
Zirconium (Zr) | ≤0.05 | Increases creep rupture strength |
Property | Value (Typical) | Test Standard/Condition |
|---|---|---|
Density | 8.2 g/cm³ | ASTM B311 |
Melting Range | 1315–1360°C | ASTM E1268 |
Thermal Conductivity | 13.3 W/m·K at 100°C | ASTM E1225 |
Electrical Resistivity | 1.08 µΩ·m at 20°C | ASTM B193 |
Thermal Expansion | 13.5 µm/m·°C (20–1000°C) | ASTM E228 |
Specific Heat Capacity | 440 J/kg·K at 20°C | ASTM E1269 |
Elastic Modulus | 200 GPa at 20°C | ASTM E111 |
Property | Value (Typical) | Test Standard |
|---|---|---|
Tensile Strength | 1100–1250 MPa | ASTM E8/E8M |
Yield Strength (0.2%) | 850–1000 MPa | ASTM E8/E8M |
Elongation | ≥20% | ASTM E8/E8M |
Hardness | 240–270 HB | ASTM E10 |
Creep Rupture Strength | 210 MPa at 800°C (1000h) | ASTM E139 |
Fatigue Resistance | Excellent | ASTM E466 |
High-Temperature Strength and Durability Nimonic PE11 retains tensile strength above 1100 MPa at 650–800°C, ensuring reliable operation in high-load environments.
Precipitation Hardening for Creep Resistance The γ′ phase strengthening mechanism provides excellent resistance to high-temperature creep and fatigue, making it ideal for turbine and engine applications.
Oxidation and Corrosion Resistance Chromium and aluminum contribute to a stable Cr₂O₃ oxide layer, ensuring long-term resistance to oxidation in environments up to 1050°C.
Good Weldability The alloy’s moderate iron content ensures weldability without the risk of hot cracking, allowing for repair and fabrication of complex parts.
Dimensional Stability With a thermal expansion coefficient of 13.5 µm/m·°C, Nimonic PE11 remains dimensionally stable under rapid thermal cycling.
The combination of high hardness and solid solution strengthening agents accelerates wear on carbide tools during machining.
Nimonic PE11’s low thermal conductivity leads to high cutting zone temperatures, increasing the risk of tool degradation and dimensional instability.
The alloy's work-hardening properties increase surface hardness during machining, requiring precise control of cutting parameters to prevent excessive tool wear.
Parameter | Recommendation | Rationale |
|---|---|---|
Tool Material | Carbide (K20–K30) or CBN inserts for finishing | High wear resistance at high temperatures |
Coating | AlTiN or TiSiN PVD (3–5 µm) | Reduces friction and heat impact on tools |
Geometry | Positive rake (6–8°), sharp cutting edge (~0.05 mm) | Minimizes cutting forces and work hardening |
Operation | Speed (m/min) | Feed (mm/rev) | Depth of Cut (mm) | Coolant Pressure (bar) |
|---|---|---|---|---|
Roughing | 10–18 | 0.10–0.20 | 2.0–3.0 | 100–120 |
Finishing | 25–35 | 0.05–0.08 | 0.3–0.8 | 120–150 |
HIP improves fatigue performance by >20%, ensuring uniform density and mechanical properties for turbine components.
Heat Treatment involves solution treatment at 1050°C followed by aging at 800°C to maximize γ′ phase formation and increase creep resistance.
Superalloy Welding ensures crack-free welds with ≥90% of base metal strength retention, even in the heat-affected zone.
TBC Coating reduces substrate temperatures by 200°C, improving the longevity of turbine blades and nozzles.
EDM provides fine details in high-precision cooling holes and internal passages with no thermal distortion.
Deep Hole Drilling achieves L/D ratios >30:1 with concentricity deviation <0.3 mm/m for deep holes required in combustion systems.
Material Testing includes tensile, creep, and fatigue testing to ensure part reliability for high-performance applications.
Aerospace Engines: Compressor blades, turbine discs, and nozzle guide vanes exposed to cyclic thermal and mechanical stresses.
Power Generation: Gas turbine blades, seals, and shafts are used in high-efficiency power cycles.
Nuclear Reactors: Pressure vessels, support brackets, and control rods are subject to both thermal and radiation stresses.
Automotive Turbo Systems: Turbocharger wheels, exhaust valves, and heat shields in high-performance engines.
Industrial Heat Treatment Equipment: Furnace fixtures, seals, and temperature-sensitive components used in high-temperature environments.