Nimonic 81 is a high-strength, nickel-chromium superalloy reinforced with aluminum and titanium, designed for excellent mechanical strength, creep resistance, and surface stability in aggressive high-temperature environments. It is precipitation-hardened and engineered for applications that demand long-term service at elevated temperatures, making it well-suited for aerospace, nuclear, and power generation components.
With a service capability of up to 870°C, Nimonic 81 combines superior thermal fatigue and high oxidation resistance. It is typically supplied in solution-annealed and aged conditions and processed through CNC machining to produce turbine blades, structural fasteners, springs, and high-precision parts requiring close dimensional tolerances and excellent surface finishes.
Nimonic 81 (UNS N07081 / W.Nr. 2.4635 / ISO 15156-3) is a precipitation-strengthened nickel alloy with a gamma-prime (γ′) phase that enhances mechanical properties under stress and thermal exposure.
Element | Composition Range (wt.%) | Key Role |
|---|---|---|
Nickel (Ni) | Balance (≥70.0) | Base element providing high-temperature oxidation and creep resistance |
Chromium (Cr) | 19.0–22.0 | Enhances corrosion and scaling resistance |
Titanium (Ti) | 2.0–2.8 | Forms Ni₃Ti γ′ phase for precipitation hardening |
Aluminum (Al) | 1.0–1.5 | Strengthens γ′ matrix for thermal fatigue resistance |
Carbon (C) | ≤0.08 | Improves high-temperature creep strength via carbide formation |
Iron (Fe) | ≤3.0 | Residual element; adds strength |
Manganese (Mn) | ≤1.0 | Supports hot workability |
Silicon (Si) | ≤1.0 | Enhances oxidation resistance |
Copper (Cu) | ≤0.2 | Limited to reduce hot shortness |
Sulfur (S) | ≤0.015 | Controlled for weldability and hot cracking resistance |
Property | Value (Typical) | Test Standard/Condition |
|---|---|---|
Density | 8.15 g/cm³ | ASTM B311 |
Melting Range | 1320–1380°C | ASTM E1268 |
Thermal Conductivity | 11.2 W/m·K at 100°C | ASTM E1225 |
Electrical Resistivity | 1.10 µΩ·m at 20°C | ASTM B193 |
Thermal Expansion | 13.2 µm/m·°C (20–1000°C) | ASTM E228 |
Specific Heat Capacity | 430 J/kg·K at 20°C | ASTM E1269 |
Elastic Modulus | 200 GPa at 20°C | ASTM E111 |
Property | Value (Typical) | Test Standard |
|---|---|---|
Tensile Strength | 1000–1150 MPa | ASTM E8/E8M |
Yield Strength (0.2%) | 700–800 MPa | ASTM E8/E8M |
Elongation | ≥18% | ASTM E8/E8M |
Hardness | 220–250 HB | ASTM E10 |
Creep Rupture Strength | 200 MPa at 750°C (1000h) | ASTM E139 |
Thermal Fatigue Life | Excellent | ASTM E606 |
High Creep Strength: Gamma-prime strengthening mechanism ensures mechanical reliability under prolonged stress at up to 870°C.
Oxidation and Scale Resistance: Chromium-enriched matrix forms a stable Cr₂O₃ scale that protects components in oxidizing atmospheres.
Fatigue Resistance Under Thermal Cycling: Maintains microstructural stability and dimensional accuracy after thousands of thermal cycles.
Good Weldability and Fabrication: It can be welded and CNC machined with controlled parameters for critical parts with tight tolerance.
Surface hardness increases rapidly during cutting, especially in aged conditions, causing tool wear and inconsistent part tolerances.
Carbides and γ′ precipitates accelerate wear on uncoated carbide and high-speed steel tooling.
Heat accumulation at the cutting edge leads to thermal softening and edge chipping of tools during dry or poorly cooled operations.
Parameter | Recommendation | Rationale |
|---|---|---|
Tool Material | Carbide (K20–K30) for roughing, CBN for finishing | Withstands abrasion and thermal loads |
Coating | AlCrN or TiSiN (3–5 µm PVD) | Reduces oxidation and BUE formation |
Geometry | Positive rake, honed edge (0.05 mm) | Minimizes cutting pressure and vibration |
Operation | Speed (m/min) | Feed (mm/rev) | Depth of Cut (mm) | Coolant Pressure (bar) |
|---|---|---|---|---|
Roughing | 10–18 | 0.20–0.25 | 1.5–2.0 | 100–120 |
Finishing | 30–45 | 0.05–0.10 | 0.3–1.0 | 120–150 |
HIP improves creep strength and structural uniformity by eliminating micro-voids in cast or AM parts.
Heat Treatment activates gamma-prime precipitation and enhances high-temperature fatigue resistance.
Superalloy Welding enables strong, oxidation-resistant joints for nuclear and aerospace hardware.
TBC Coating adds thermal protection to turbine blades, combustion rings, and hot gas hardware.
EDM ensures precision on hardened features such as cooling holes, notches, or sealing surfaces.
Deep Hole Drilling supports the manufacturing of coolant passages or injector channels with high length-to-diameter ratios.
Material Testing includes microhardness profiling, grain size analysis, stress rupture testing, and non-destructive inspection (NDT).
Turbine disks, blade roots, and combustion chamber details exposed to high heat and cyclic stress.
Fuel rod spacers, bolting, and springs operate under neutron flux and elevated pressure.
Fasteners, heat exchanger supports, and turbine seals operating above 700°C.