English

Nimonic 80A

Nimonic 80A is a high-strength, precipitation-hardened nickel-chromium alloy ideal for CNC-machined parts in extreme heat and fatigue environments. It offers excellent oxidation resistance, creep life, and dimensional stability for aerospace and power systems.

Introduction to Nimonic 80A

Nimonic 80A is a precipitation-hardened nickel-chromium alloy strengthened with titanium and aluminum, engineered for use in high-temperature environments where exceptional mechanical strength, creep resistance, and oxidation resistance are critical. It offers improved high-temperature strength over Nimonic 75 and maintains structural integrity in continuous service up to 815°C and intermittent exposure beyond 1000°C.

Its excellent thermal fatigue and corrosion resistance make it a preferred material for aerospace turbines, nuclear valves, high-pressure springs, and automotive turbocharger components. Components made from Nimonic 80A are frequently manufactured by forging or casting and precision-finished through CNC machining for tight-tolerance performance-critical applications.


Chemical, Physical, and Mechanical Properties of Nimonic 80A

Nimonic 80A (UNS N07080 / W.Nr. 2.4952 / ASTM B637, B408) is a gamma-prime (γ') strengthened alloy designed for high-temperature strength, oxidation resistance, and structural reliability in creep and fatigue-prone environments.

Chemical Composition (Typical)

Element

Composition Range (wt.%)

Key Role

Nickel (Ni)

Balance (≥69.0)

Matrix providing oxidation resistance and thermal strength

Chromium (Cr)

18.0–21.0

Forms a protective oxide scale; enhances corrosion resistance

Titanium (Ti)

1.8–2.7

Precipitation hardening through γ'-Ni₃(Al,Ti) formation

Aluminum (Al)

1.0–1.8

Strengthens the alloy via gamma-prime phase

Iron (Fe)

≤3.0

Residual element

Carbon (C)

≤0.10

Controls carbide precipitation and creep behavior

Manganese (Mn)

≤1.0

Improves hot workability

Silicon (Si)

≤1.0

Enhances oxidation resistance and casting properties

Copper (Cu)

≤0.2

Limited to minimize hot shortness

Sulfur (S)

≤0.015

Controlled to reduce hot cracking in welding


Physical Properties

Property

Value (Typical)

Test Standard/Condition

Density

8.19 g/cm³

ASTM B311

Melting Range

1320–1380°C

ASTM E1268

Thermal Conductivity

11.4 W/m·K at 100°C

ASTM E1225

Electrical Resistivity

1.08 µΩ·m at 20°C

ASTM B193

Thermal Expansion

13.3 µm/m·°C (20–1000°C)

ASTM E228

Specific Heat Capacity

435 J/kg·K at 20°C

ASTM E1269

Elastic Modulus

200 GPa at 20°C

ASTM E111


Mechanical Properties (Solution Treated + Aged)

Property

Value (Typical)

Test Standard

Tensile Strength

965–1080 MPa

ASTM E8/E8M

Yield Strength (0.2%)

690–760 MPa

ASTM E8/E8M

Elongation

≥20%

ASTM E8/E8M

Hardness

200–230 HB

ASTM E10

Creep Rupture Strength

180 MPa at 750°C (1000h)

ASTM E139

Fatigue Resistance

Excellent

ASTM E466


Key Characteristics of Nimonic 80A

  • High-Temperature Strength: Precipitation of Ni₃(Al,Ti) phase allows high tensile and creep strength up to 815°C in continuous service.

  • Oxidation Resistance: Retains mechanical properties in oxidizing environments, even with intermittent exposure above 1000°C.

  • Excellent Fatigue and Thermal Shock Resistance: Suitable for turbine and spring applications under cyclic thermal and mechanical stress.

  • Enhanced Creep and Rupture Life: Particularly suitable for bolting, valve guides, and pressure-sealing parts in turbines and reactors.


CNC Machining Challenges and Solutions for Nimonic 80A

Machining Challenges

Work Hardening

  • Precipitation-hardened structure increases surface hardness rapidly, causing premature tool wear and potential tolerance issues.

Reduced Tool Life

  • High-temperature strength and abrasion from intermetallic phases like γ'-Ni₃(Al,Ti) cause flank wear and crater formation in carbide tools.

Heat Generation

  • Limited thermal conductivity leads to poor heat dissipation, increasing the likelihood of thermal cracking and edge deformation.


Optimized Machining Strategies

Tool Selection

Parameter

Recommendation

Rationale

Tool Material

Fine-grain carbide (K20–K30), or CBN for finishing

High wear resistance under thermal stress

Coating

AlTiN or TiSiN (3–5 µm PVD)

Improves tool life by resisting oxidation and adhesion

Geometry

Positive rake, sharp cutting edge, 0.05 mm edge hone

Reduces cutting forces and prevents edge chipping

Cutting Parameters (ISO 3685 Compliant)

Operation

Speed (m/min)

Feed (mm/rev)

Depth of Cut (mm)

Coolant Pressure (bar)

Roughing

12–20

0.15–0.20

1.5–2.5

100–120

Finishing

30–45

0.05–0.10

0.2–1.0

120–150


Surface Treatment for Machined Nimonic 80A Parts

Hot Isostatic Pressing (HIP)

HIP enhances fatigue life and dimensional stability by eliminating internal porosity in cast or AM components.

Heat Treatment

Heat Treatment stabilizes the gamma-prime phase and optimizes mechanical properties for high-stress, high-temperature conditions.

Superalloy Welding

Superalloy Welding using matching filler material ensures integrity in pressure-bound joints or assemblies.

Thermal Barrier Coating (TBC)

TBC Coating provides protection for turbine and exhaust parts operating above 900°C.

Electrical Discharge Machining (EDM)

EDM achieves sub-10 µm tolerances on heat-treated surfaces without introducing residual stresses.

Deep Hole Drilling

Deep Hole Drilling for manufacturing internal features in bolts, springs, and fuel lines with L/D > 20:1.

Material Testing and Analysis

Material Testing includes tensile testing, creep life, microstructure validation, and ultrasonic or penetrant inspection.


Industry Applications of Nimonic 80A Components

Aerospace Turbine Systems

  • Turbine blades, combustion components, seals, and nozzle vanes operating in thermal cycling environments.

Nuclear and Power Generation

  • Valve spindles, control rods, and guide sleeves in reactors requiring long-term mechanical and creep stability.

Automotive Turbocharger Systems

  • Springs, brackets, and housings subjected to fluctuating thermal and mechanical loads.

Industrial Furnaces and Heat Treatment

  • Retorts, hangers, and grates exposed to oxidizing or carburizing atmospheres up to 1000°C.