Monel R-405

A free-machining nickel-copper alloy engineered for automated turning and screw machining of corrosion-resistant components. Ideal for CNC production of marine, chemical, and oil & gas threaded parts.

Introduction to Monel R-405

Monel R-405 is a free-machining version of the widely used Monel 400 nickel-copper alloy. Developed specifically for high-speed machining operations, Monel R-405 contains controlled sulfur additions to improve chip breaking and machinability without compromising the alloy’s excellent corrosion resistance.

Designed for high-volume production of threaded, precision, or valve components, Monel R-405 maintains good mechanical properties and seawater resistance while offering significantly better tool life and surface finish in CNC turning and automatic screw machine operations. It is commonly used in marine fittings, oil & gas tools, pump components, and electrical connectors.


Chemical, Physical, and Mechanical Properties of Monel R-405

Monel R-405 (UNS N04405 / ASTM B164) is a solid-solution nickel-copper alloy modified with sulfur to improve machinability. It is supplied in annealed or stress-relieved conditions to maximize its manufacturing performance.

Chemical Composition (Typical)

Element

Composition Range (wt.%)

Key Role

Nickel (Ni)

≥63.0

Base element; corrosion resistance and toughness

Copper (Cu)

28.0–34.0

Enhances resistance to acids and seawater

Sulfur (S)

0.025–0.060

Improves machinability by promoting chip breakage

Iron (Fe)

≤2.5

Strengthens the alloy

Manganese (Mn)

≤2.0

Improves hot workability

Silicon (Si)

≤0.5

Improves oxidation resistance

Carbon (C)

≤0.3

Kept low to preserve weldability


Physical Properties

Property

Value (Typical)

Test Standard/Condition

Density

8.80 g/cm³

ASTM B311

Melting Range

1300–1350°C

ASTM E1268

Thermal Conductivity

22.0 W/m·K at 100°C

ASTM E1225

Electrical Resistivity

0.43 µΩ·m at 20°C

ASTM B193

Thermal Expansion

13.9 µm/m·°C (20–300°C)

ASTM E228

Specific Heat Capacity

427 J/kg·K at 20°C

ASTM E1269

Elastic Modulus

179 GPa at 20°C

ASTM E111


Mechanical Properties (Annealed Condition)

Property

Value (Typical)

Test Standard

Tensile Strength

480–620 MPa

ASTM E8/E8M

Yield Strength (0.2%)

170–275 MPa

ASTM E8/E8M

Elongation

≥30% (25mm gauge)

ASTM E8/E8M

Hardness

120–180 HB

ASTM E10

Impact Toughness

Excellent at sub-zero temperatures

ASTM E23


Key Characteristics of Monel R-405

  • Enhanced Machinability: Sulfur content ensures shorter, curled chips that reduce tool loading and extend tool life by 25–40% over Monel 400.

  • Corrosion Resistance: Comparable to Monel 400 in seawater, brine, sulfuric acid, and hydrofluoric acid environments.

  • Non-Magnetic Stability: Remains non-magnetic in all processed forms, ideal for use near sensitive instrumentation.

  • High-Rate Machining Compatibility: Optimized for CNC lathes, screw machines, and high-speed precision turning of small components.


CNC Machining Challenges and Solutions for Monel R-405

Machining Challenges

Tool Abrasion

  • While more machinable than Monel 400, the material’s strength still causes moderate flank wear at high speeds without appropriate tooling.

Sulfide Inclusion Effects

  • Sulfur improves machinability but can slightly reduce weldability and surface polish capability if not properly managed during finishing.

Chip Control in High-Feed Applications

  • At excessive feed rates, chip evacuation must be assisted with aggressive coolant delivery and sharp tool profiles.


Optimized Machining Strategies

Tool Selection

Parameter

Recommendation

Rationale

Tool Material

Cobalt HSS or uncoated carbide

Maximizes edge retention for short runs

Coating

TiN or TiCN (2–3 µm)

Reduces galling and improves chip release

Geometry

10–12° rake, sharp nose radius (0.4–0.8 mm)

Enhances surface finish and reduces work hardening

Cutting Parameters (ISO 3685)

Operation

Speed (m/min)

Feed (mm/rev)

DOC (mm)

Coolant Pressure (bar)

Roughing

30–50

0.20–0.30

2.0–3.0

80–100

Finishing

50–80

0.05–0.10

0.5–1.0

100–120


Surface Treatment for Machined Monel R-405 Parts

Hot Isostatic Pressing (HIP)

HIP is rarely required for Monel R-405 but can be applied for critical castings to enhance fatigue life and density.

Heat Treatment

Heat Treatment includes annealing at 850–900°C followed by controlled cooling to maintain machining-friendly microstructure.

Superalloy Welding

Superalloy Welding is not recommended due to sulfur content; if needed, Monel 400 is preferred for weld-compatible assemblies.

Thermal Barrier Coating (TBC)

TBC Coating is not common but may be used in high-temperature fittings requiring thermal shock protection.

Electrical Discharge Machining (EDM)

EDM is well suited for precision slotting, threads, and intricate features in Monel R-405 without mechanical stress.

Deep Hole Drilling

Deep Hole Drilling enables internal flow or alignment channels in compact oil & gas or marine parts.

Material Testing and Analysis

Material Testing includes conductivity verification, microstructure analysis, sulfur distribution mapping, and mechanical property validation.


Industry Applications of Monel R-405 Components

Marine and Subsea

  • Shaft sleeves, valves, and seawater fittings.

  • Excellent resistance to flow-induced corrosion in brine and saltwater systems.

Oil & Gas

  • Threaded tool components, connectors, instrument housings.

  • Ideal for automated machining of large-volume precision parts in sour environments.

Chemical Processing

  • Pump shafts, fasteners, acid-resistant couplings.

  • Suitable for use in hydrofluoric acid and sulfur-rich processing lines.

Electrical and Instrumentation

  • Terminal pins, switch housings, and EMI-resistant mounts.

  • Non-magnetic and corrosion-resistant features support precision assemblies.