A high-strength, precipitation-hardened nickel-copper alloy combining excellent seawater corrosion resistance with superior mechanical properties. Ideal for CNC-machined parts in subsea, oilfield, and aerospace systems requiring toughness and durability.

Introduction to Monel K500

Monel K500 is a high-strength, precipitation-hardenable nickel-copper alloy that offers the same outstanding corrosion resistance as Monel 400, but with significantly enhanced mechanical properties. The addition of aluminum and titanium enables age hardening, increasing tensile and yield strength while maintaining resistance to chloride stress corrosion cracking and seawater environments.

Monel K500 is especially valued in CNC machining for critical parts in aerospace, marine, petroleum, and chemical processing industries. Its ability to retain strength and ductility across temperatures ranging from cryogenic to 650°C makes it a top choice for fasteners, pump shafts, and non-magnetic components operating under high stress or flow conditions.


Chemical, Physical, and Mechanical Properties of Monel K500

Monel K500 (UNS N05500 / ASTM B865 / AMS 4676) is a wrought, nickel-copper-aluminum alloy strengthened through precipitation of γ′ (Ni₃(Al,Ti)) phases during aging. It is available in solution-annealed, aged, and hot-worked conditions.

Chemical Composition (Typical)

Element

Composition Range (wt.%)

Key Role

Nickel (Ni)

≥63.0

Base element; provides corrosion resistance

Copper (Cu)

27.0–33.0

Improves seawater and acid resistance

Aluminum (Al)

2.30–3.15

Enables precipitation strengthening (γ′ phase)

Titanium (Ti)

0.35–0.85

Enhances aging response and strength

Iron (Fe)

≤2.0

Maintains toughness and cost efficiency

Manganese (Mn)

≤1.5

Improves hot workability

Silicon (Si)

≤0.5

Enhances oxidation resistance

Carbon (C)

≤0.25

Controlled to prevent carbide precipitation

Sulfur (S)

≤0.01

Reduced to avoid hot cracking and inclusion defects


Physical Properties

Property

Value (Typical)

Test Standard/Condition

Density

8.44 g/cm³

ASTM B311

Melting Range

1315–1350°C

ASTM E1268

Thermal Conductivity

17.0 W/m·K at 100°C

ASTM E1225

Electrical Resistivity

0.43 µΩ·m at 20°C

ASTM B193

Thermal Expansion

13.8 µm/m·°C (20–300°C)

ASTM E228

Specific Heat Capacity

410 J/kg·K at 20°C

ASTM E1269

Elastic Modulus

179 GPa at 20°C

ASTM E111


Mechanical Properties (Aged Condition)

Property

Value (Typical)

Test Standard

Tensile Strength

960–1100 MPa

ASTM E8/E8M

Yield Strength (0.2%)

690–860 MPa

ASTM E8/E8M

Elongation

≥20% (25mm gauge)

ASTM E8/E8M

Hardness

28–35 HRC

ASTM E18

Impact Toughness

≥100 J at -150°C

ASTM E23


Key Characteristics of Monel K500

  • High Strength via Aging: Compared to Monel 400, tensile strength increases by 2× to 3× due to γ′ phase precipitation, reaching values up to 1100 MPa.

  • Excellent Corrosion Resistance: Maintains low corrosion rates (e.g., <0.05 mm/year) in 3.5% NaCl at 25°C and hydrofluoric acid solutions, even under flow conditions exceeding 15 m/s.

  • Seawater Resistance: Resists cavitation and erosion in high-velocity brine environments, ideal for marine pump impellers and shafts.

  • Non-Magnetic Stability: Remains essentially non-magnetic in solution-annealed condition; may show slight magnetism after aging, acceptable for most non-magnetic assemblies.

  • Thermal Range: Operational stability from cryogenic temperatures up to 650°C; minimal creep deformation below 0.5% strain at 450°C over 10,000 hours.


CNC Machining Challenges and Solutions for Monel K500

Machining Challenges

High Hardness After Aging

  • Hardness values up to 35 HRC cause flank wear and edge chipping in conventional tools, requiring premium-grade carbide inserts.

Rapid Work Hardening

  • Increases local hardness by 20–30% under shallow cuts, risking tool deflection and poor surface finish if tool geometry is not optimized.

Chip Formation and Heat Retention

  • Produces continuous, adhesive chips that raise cutting zone temperatures above 600°C, especially in dry conditions, reducing tool life.


Optimized Machining Strategies

Tool Selection

Parameter

Recommendation

Rationale

Tool Material

PVD-coated carbide (K10–K20 grade) or ceramic inserts

Maintains wear resistance at elevated temperatures

Coating

AlTiN, TiAlN, or AlCrN (2–4 µm)

Reduces friction and thermal loading

Geometry

Positive rake (10–12°), honed edge (~0.02 mm radius)

Reduces cutting force and chip adhesion

Cutting Parameters (ISO 3685)

Operation

Speed (m/min)

Feed (mm/rev)

DOC (mm)

Coolant Pressure (bar)

Roughing

15–25

0.20–0.30

2.0–3.0

100–120

Finishing

30–50

0.05–0.10

0.5–1.0

120–150


Surface Treatment for Machined Monel K500 Parts

Hot Isostatic Pressing (HIP)

HIP eliminates internal porosity and increases fatigue strength (>20%) for high-pressure service components.

Heat Treatment

Heat Treatment includes solution annealing at 980°C ±10°C for 2 hours and aging at 595°C for 8–16 hours to achieve full precipitation hardening.

Superalloy Welding

Superalloy Welding uses controlled heat input and post-weld aging to recover mechanical properties, especially for pressure-retaining parts.

Thermal Barrier Coating (TBC)

TBC Coating applies up to 200 µm of YSZ ceramic for gas turbine applications, enabling service up to 1000°C on exhaust components.

Electrical Discharge Machining (EDM)

EDM allows for micro-slotting and feature detailing on hardened K500 with ±0.005 mm tolerance control.

Deep Hole Drilling

Deep Hole Drilling creates coolant or oil channels up to 50× diameter in pump shafts or marine rotors.

Material Testing and Analysis

Material Testing includes hardness mapping, X-ray diffraction (XRD) for phase analysis, corrosion testing (ASTM G28), and tensile testing (ASTM E8).


Industry Applications of Monel K500 Components

Marine and Subsea

  • Pump shafts, valve stems, and underwater fasteners.

  • Corrosion rate in seawater: <0.02 mm/year at 25°C with flow rates >10 m/s.

Oil & Gas

  • Non-magnetic drill collars, completion tools, and wellhead hardware.

  • Meets NACE MR0175 standards for H₂S service with tensile strength >960 MPa.

Aerospace

  • Actuator parts, landing gear bushings, fastening systems.

  • Withstands cyclic loads and vibration fatigue up to 10⁷ cycles without failure.

Chemical and Power Plants

  • Corrosion-resistant seals, impellers, and HF acid-handling parts.

  • Maintains mechanical integrity in pH 1–13 environments at up to 150°C.