English

Monel 404

A low-resistivity, corrosion-resistant nickel-copper alloy optimized for precision electrical components in marine, electronic, and signal-critical applications. Ideal for CNC-machined low-voltage terminals and instrumentation housings.

Introduction to Monel 404

Monel 404 is a low-resistivity, nickel-copper alloy developed specifically for electrical and electronic applications where consistent conductivity, good corrosion resistance, and moderate strength are required. With a nominal composition of approximately 52% nickel and 48% copper, Monel 404 provides excellent performance in communication systems, marine electronics, and precision control devices.

Unlike other Monel grades, Monel 404 is optimized for low electrical resistance and ease of formability. It is often CNC machined in the annealed state to produce high-precision connectors, terminal pins, sensor housings, and other tight-tolerance components used in low-voltage or signal-sensitive environments.


Chemical, Physical, and Mechanical Properties of Monel 404

Monel 404 (UNS N04404 / ASTM B164) is a wrought nickel copper alloy designed to deliver electrical conductivity and corrosion resistance without magnetic interference. It is non-heat-treatable and is typically strengthened through cold working.

Chemical Composition (Typical)

Element

Composition Range (wt.%)

Key Role

Nickel (Ni)

52.0–57.0

Base metal; provides corrosion resistance and ductility

Copper (Cu)

43.0–48.0

Lowers resistivity and enhances seawater resistance

Iron (Fe)

≤0.5

Maintained low for high conductivity and ductility

Manganese (Mn)

≤0.1

Controlled to minimize residual magnetic response

Silicon (Si)

≤0.1

Stabilizes electrical properties under thermal load

Carbon (C)

≤0.1

Reduced to avoid grain boundary embrittlement

Sulfur (S)

≤0.024

Minimized to prevent inclusions and surface cracking


Physical Properties

Property

Value (Typical)

Test Standard/Condition

Density

8.89 g/cm³

ASTM B311

Melting Range

1240–1290°C

ASTM E1268

Thermal Conductivity

23.0 W/m·K at 100°C

ASTM E1225

Electrical Resistivity

0.33 µΩ·m at 20°C

ASTM B193

Magnetic Permeability

<1.01 (relative)

ASTM A342

Thermal Expansion

13.8 µm/m·°C (20–300°C)

ASTM E228

Specific Heat Capacity

420 J/kg·K at 20°C

ASTM E1269

Elastic Modulus

176 GPa at 20°C

ASTM E111


Mechanical Properties (Annealed Condition)

Property

Value (Typical)

Test Standard

Tensile Strength

410–540 MPa

ASTM E8/E8M

Yield Strength (0.2%)

120–200 MPa

ASTM E8/E8M

Elongation

≥35% (25mm gauge)

ASTM E8/E8M

Hardness

110–150 HB

ASTM E10

Impact Toughness

Excellent at cryogenic temperatures

ASTM E23


Key Characteristics of Monel 404

  • Low Electrical Resistivity: With a resistivity of only 0.33 µΩ·m, it is ideal for electrical connectors and signal-transmitting components.

  • Corrosion Resistance: Performs well in marine, salt-spray, and mildly acidic environments, offering longevity in coastal or submerged systems.

  • Non-Magnetic: Stable performance in electromagnetic-sensitive equipment such as radar, sensors, and relay housings.

  • CNC Machinability: Capable of producing high-precision components with tight tolerances (±0.01 mm) and surface finishes below Ra 1.0 µm.


CNC Machining Challenges and Solutions for Monel 404

Machining Challenges

High Ductility and Adhesion

  • The alloy’s softness can lead to smearing and built-up edge (BUE) formation, especially at low feed rates or dull tooling.

Chip Control

  • Produces long, stringy chips during turning or drilling, requiring chip breakers and optimized tool geometry.

Tolerance Sensitivity

  • Used in precision electronics; parts must maintain consistent tolerances, especially in threaded or contact surfaces.


Optimized Machining Strategies

Tool Selection

Parameter

Recommendation

Rationale

Tool Material

Fine-grain carbide or cobalt HSS

Maintains edge sharpness during long machining cycles

Coating

TiN or TiCN (2–3 µm)

Minimizes galling and adhesive wear

Geometry

Sharp rake with polished flutes

Enhances chip flow and surface quality

Cutting Parameters (ISO 3685)

Operation

Speed (m/min)

Feed (mm/rev)

DOC (mm)

Coolant Pressure (bar)

Roughing

25–40

0.20–0.30

1.5–2.0

60–90

Finishing

45–70

0.05–0.10

0.3–0.8

90–120


Surface Treatment for Machined Monel 404 Parts

Hot Isostatic Pressing (HIP)

HIP is rarely needed for Monel 404 but may be applied to improve density and surface uniformity for electronic-grade castings.

Heat Treatment

Heat Treatment typically includes annealing at 850–900°C followed by controlled air cooling to maintain electrical and mechanical consistency.

Superalloy Welding

Superalloy Welding allows Monel 404 parts to be joined with minimal magnetic or resistivity change using ERNiCu-7 filler.

Thermal Barrier Coating (TBC)

TBC Coating is not typically applied, but anti-corrosion or anti-static coatings can be used for electronics in humid conditions.

Electrical Discharge Machining (EDM)

EDM supports ultra-fine features in terminals, relays, and sockets with micro-tolerance control.

Deep Hole Drilling

Deep Hole Drilling is suitable for forming internal signal paths or cable channels in complex housing geometries.

Material Testing and Analysis

Material Testing includes electrical conductivity verification, permeability testing (ASTM A342), tensile testing, and surface quality analysis.


Industry Applications of Monel 404 Components

Electronics and Communications

  • Relay housings, electrical connectors, coaxial contacts, and waveguide shields.

  • Reliable performance in low-voltage, signal-transmission, and EMI-sensitive circuits.

Marine Electronics

  • Saltwater connectors, underwater instrumentation, and sonar control housings.

  • Excellent salt spray and seawater resistance with low maintenance.

Instrumentation

  • Precision terminals, thermocouple cases, and magnetic shielding components.

  • Suitable for analytical and control devices operating under variable temperatures.

Aerospace Systems

  • EMI enclosures, lightweight electrical fittings, and cryogenic controls.

  • Maintains conductivity and dimensional integrity across thermal cycling.