Monel 401

A low-permeability nickel-copper alloy engineered for electrical and marine applications requiring corrosion resistance and stable conductivity. Ideal for CNC-machined components in instrumentation and sensor systems.

Introduction to Monel 401

Monel 401 is a binary nickel-copper alloy engineered specifically for electrical and electronic applications requiring high permeability and low electrical resistivity. With a composition closely related to Monel 400 but with narrower tolerances, Monel 401 offers improved magnetic properties, consistent mechanical behavior, and superior corrosion resistance in various environments.

This alloy is ideally suited for manufacturing high-integrity electrical connectors, relay cores, and control instrumentation components. CNC machining of Monel 401 is typically performed in its annealed state to achieve fine-tolerance control and smooth finishes without compromising magnetic or corrosion performance.


Chemical, Physical, and Mechanical Properties of Monel 401

Monel 401 (UNS N04401 / ASTM B164) is a wrought nickel-copper alloy designed for electrical applications, offering moderate strength, excellent corrosion resistance, and low magnetic permeability.

Chemical Composition (Typical)

Element

Composition Range (wt.%)

Key Role

Nickel (Ni)

45.0–52.0

Base element; controls electrical/magnetic properties

Copper (Cu)

47.0–52.0

Enhances corrosion resistance and stabilizes the structure

Iron (Fe)

≤2.0

Provides strength without sacrificing magnetic neutrality

Manganese (Mn)

≤2.0

Supports hot workability and grain refinement

Silicon (Si)

≤0.5

Aids in oxidation resistance

Carbon (C)

≤0.15

Maintained low for consistent conductivity

Sulfur (S)

≤0.024

Minimized to prevent hot cracking in manufacturing


Physical Properties

Property

Value (Typical)

Test Standard/Condition

Density

8.80 g/cm³

ASTM B311

Melting Range

1300–1350°C

ASTM E1268

Thermal Conductivity

21.5 W/m·K at 100°C

ASTM E1225

Electrical Resistivity

0.50 µΩ·m at 20°C

ASTM B193

Magnetic Permeability

<1.01 (relative)

ASTM A342

Thermal Expansion

13.6 µm/m·°C (20–300°C)

ASTM E228

Specific Heat Capacity

420 J/kg·K at 20°C

ASTM E1269

Elastic Modulus

177 GPa at 20°C

ASTM E111


Mechanical Properties (Annealed Condition)

Property

Value (Typical)

Test Standard

Tensile Strength

420–550 MPa

ASTM E8/E8M

Yield Strength (0.2%)

140–210 MPa

ASTM E8/E8M

Elongation

≥30% (25mm gauge)

ASTM E8/E8M

Hardness

110–150 HB

ASTM E10

Impact Toughness

Excellent at cryogenic temperatures

ASTM E23


Key Characteristics of Monel 401

  • Low Magnetic Permeability: Ideal for precision instrumentation, signal shielding, and components in magnetic-sensitive systems.

  • Stable Electrical Resistivity: Uniform conductivity with low variation across temperature ranges—suitable for connectors and terminals.

  • Excellent Corrosion Resistance: Resists attack from seawater, salt spray, and moderate acids, making it viable in marine and coastal systems.

  • CNC Machinability: Maintains dimensional accuracy in small-scale or tight-tolerance parts, even after annealing and surface processing.


CNC Machining Challenges and Solutions for Monel 401

Machining Challenges

Work Hardening Tendency

  • Like other Monel alloys, Monel 401 work-hardens quickly, making it necessary to use aggressive feeds and depths of cut to avoid surface hardening.

Tool Adhesion and Chip Formation

  • Tends to form built-up edge (BUE) and long, continuous chips, which can affect tool life and surface finish if not controlled.

Dimensional Control in Small Parts

  • Precision electrical parts require ±0.01 mm tolerances, necessitating stable fixturing and proper coolant application to control thermal effects.


Optimized Machining Strategies

Tool Selection

Parameter

Recommendation

Rationale

Tool Material

PVD-coated carbide or cobalt HSS

Provides balance of wear resistance and edge retention

Coating

TiN or TiCN (2–3 µm)

Minimizes adhesion and improves chip evacuation

Geometry

High positive rake with polished finish

Ensures chip flow and avoids surface tearing

Cutting Parameters (ISO 3685)

Operation

Speed (m/min)

Feed (mm/rev)

DOC (mm)

Coolant Pressure (bar)

Roughing

20–35

0.15–0.25

1.5–2.5

50–80

Finishing

40–60

0.05–0.10

0.3–0.8

80–120


Surface Treatment for Machined Monel 401 Parts

Hot Isostatic Pressing (HIP)

HIP is not commonly applied to Monel 401, but may be used for densification in critical cast components.

Heat Treatment

Heat Treatment includes annealing at 850–900°C with air cooling to optimize mechanical and magnetic uniformity.

Superalloy Welding

Superalloy Welding supports Monel 401 using GTAW and compatible Ni-Cu filler (ERNiCu-7), minimizing distortion and magnetic degradation.

Thermal Barrier Coating (TBC)

TBC Coating is generally not required, but selective anti-corrosion or insulation coatings can be applied for marine electronics.

Electrical Discharge Machining (EDM)

EDM supports fabrication of micro-features and tight-tolerance electronic profiles, down to ±0.005 mm.

Deep Hole Drilling

Deep Hole Drilling enables formation of terminal pathways and fine tubular passageways in relay and signal transmission devices.

Material Testing and Analysis

Material Testing includes conductivity testing, magnetic permeability (ASTM A342), tensile strength validation, and salt spray testing (ASTM B117).


Industry Applications of Monel 401 Components

Electrical and Instrumentation

  • Relay cores, switch terminals, signal shielding enclosures, and wiring connectors.

  • Offers dimensional and conductivity stability in magnetic-sensitive environments.

Marine Electronics

  • Saltwater-resistant enclosures, transducer mounts, and underwater sensor casings.

  • Resists galvanic corrosion in seawater-exposed electronics.

Aerospace

  • Electronic housings, EMI/RFI shields, and cryogenic connectors.

  • Maintains mechanical and electrical properties across altitude and temperature variations.

Scientific Equipment

  • Low-magnetic parts for mass spectrometers, analytical probes, and MRI systems.

  • Stable performance in sensitive electromagnetic conditions.