Monel 400

A high-strength, corrosion-resistant nickel-copper alloy ideal for CNC-machined components in marine, chemical, and sour gas service. Maintains toughness and dimensional stability across a wide temperature range.

Introduction to Monel 400

Monel 400 is a solid-solution nickel-copper alloy known for its exceptional corrosion resistance, high strength, and good weldability. With a nominal composition of 67% nickel and 30% copper, it offers outstanding performance in marine and chemical environments, particularly where resistance to acidic and alkaline media, saltwater, and hydrofluoric acid is critical.

Monel 400 maintains structural integrity from cryogenic temperatures up to 550°C and exhibits good toughness across this range. The alloy is often CNC machined in annealed condition to ensure stability and tight tolerance control for critical components such as valves, shafts, fittings, and heat exchanger parts.


Chemical, Physical, and Mechanical Properties of Monel 400

Monel 400 (UNS N04400 / ASTM B164 / AMS 4675) is non-hardenable by heat treatment and relies on cold working for strengthening. It is delivered in annealed, stress-relieved, or cold-drawn condition depending on application demands.

Chemical Composition (Typical)

Element

Composition Range (wt.%)

Key Role

Nickel (Ni)

≥63.0

Base metal for corrosion resistance and ductility

Copper (Cu)

28.0–34.0

Enhances resistance to acids and seawater

Iron (Fe)

≤2.5

Strengthens the alloy without compromising corrosion resistance

Manganese (Mn)

≤2.0

Improves hot workability

Silicon (Si)

≤0.5

Enhances oxidation resistance

Carbon (C)

≤0.3

Controlled to maintain weldability

Sulfur (S)

≤0.024

Minimized to prevent hot cracking


Physical Properties

Property

Value (Typical)

Test Standard/Condition

Density

8.80 g/cm³

ASTM B311

Melting Range

1300–1350°C

ASTM E1268

Thermal Conductivity

22.0 W/m·K at 100°C

ASTM E1225

Electrical Resistivity

0.43 µΩ·m at 20°C

ASTM B193

Thermal Expansion

13.9 µm/m·°C (20–300°C)

ASTM E228

Specific Heat Capacity

427 J/kg·K at 20°C

ASTM E1269

Elastic Modulus

179 GPa at 20°C

ASTM E111


Mechanical Properties (Annealed Condition)

Property

Value (Typical)

Test Standard

Tensile Strength

480–620 MPa

ASTM E8/E8M

Yield Strength (0.2%)

170–280 MPa

ASTM E8/E8M

Elongation

≥35% (25mm gauge)

ASTM E8/E8M

Hardness

120–180 HB

ASTM E10

Impact Toughness

Excellent at -196°C

ASTM E23


Key Characteristics of Monel 400

  • Excellent Corrosion Resistance: Withstands hydrofluoric acid, seawater, sulfuric acid, and alkali environments—ideal for marine and chemical process systems.

  • Non-Magnetic and Cryogenic Stability: Maintains toughness at sub-zero temperatures, making it suitable for liquefied gas equipment.

  • Good Machinability: While work-hardening, it offers stable performance during CNC turning and milling, especially with proper tooling and coolant strategies.

  • Weldability: Easily welded using gas tungsten arc, gas metal arc, and resistance welding methods, without post-weld cracking.


CNC Machining Challenges and Solutions for Monel 400

Machining Challenges

Work Hardening Tendency

  • Rapid work hardening requires consistent depth of cut to avoid excessive tool wear and dimensional drift.

BUE and Tool Wear

  • Prone to built-up edge (BUE), leading to surface finish degradation and unpredictable chip formation.

Low Thermal Conductivity

  • Generates localized heat zones at the tool-workpiece interface, especially during drilling and threading.


Optimized Machining Strategies

Tool Selection

Parameter

Recommendation

Rationale

Tool Material

Carbide tools or high-speed steel (HSS-Co)

Maintains sharpness and wear resistance

Coating

TiAlN or TiCN (2–3 µm)

Reduces BUE formation and thermal stress

Geometry

10–12° rake with polished flutes

Enhances chip evacuation and cutting consistency

Cutting Parameters (ISO 3685)

Operation

Speed (m/min)

Feed (mm/rev)

DOC (mm)

Coolant Pressure (bar)

Roughing

20–35

0.20–0.30

2.0–3.0

50–80

Finishing

40–60

0.05–0.15

0.5–1.0

80–120


Surface Treatment for Machined Monel 400 Parts

Hot Isostatic Pressing (HIP)

HIP is rarely used for Monel 400 but can be applied to improve internal soundness in cast or additively manufactured parts.

Heat Treatment

Heat Treatment typically includes annealing at 850–900°C followed by controlled cooling to relieve residual stresses.

Superalloy Welding

Superalloy Welding allows Monel 400 to be joined without cracking, using Ni-Cu filler metals (ERNiCu-7).

Thermal Barrier Coating (TBC)

TBC Coating is not commonly used, but corrosion-resistant coatings may be applied for seawater or acidic service.

Electrical Discharge Machining (EDM)

EDM is ideal for producing precision grooves, slots, and cavities in hardened or thin-walled Monel 400 components.

Deep Hole Drilling

Deep Hole Drilling enables internal coolant paths or threaded bores in marine pump shafts and valve bodies.

Material Testing and Analysis

Material Testing includes salt spray testing (ASTM B117), mechanical property verification, and grain size inspection per ASTM E112.


Industry Applications of Monel 400 Components

Marine Engineering

  • Pump shafts, propeller shafts, seawater valves, and fasteners.

  • Outstanding resistance to biofouling, salt spray, and brine environments.

Chemical Processing

  • Acid-handling tanks, heat exchangers, agitators, and process piping.

  • Performs well in hydrochloric, sulfuric, and hydrofluoric acid conditions.

Oil & Gas

  • Downhole tools, valves, and instrumentation exposed to sour gas.

  • Complies with NACE MR0175 for H₂S resistance in corrosive wells.

Aerospace and Cryogenics

  • Fuel system components, cryogenic valves, and brackets.

  • Maintains strength and impact resistance at temperatures as low as −200°C.