Inconel X-750

A high-strength, corrosion- and oxidation-resistant nickel-chromium alloy ideal for CNC-machined turbine, nuclear, and aerospace components exposed to sustained or cyclic high-temperature conditions.

Introduction to Inconel X-750

Inconel X-750 is a precipitation-hardenable nickel-chromium alloy renowned for its exceptional high-temperature strength, oxidation resistance, and stress-corrosion cracking resistance. Strengthened through gamma prime (γ′) precipitation via aluminum and titanium additions, this alloy offers stable mechanical properties at temperatures up to 700°C and intermittent exposure up to 980°C.

With its origins in jet engine and nuclear applications, Inconel X-750 is widely used for springs, fasteners, gas turbine blades, and pressure vessel components. It is available in wrought and cast forms and is typically CNC machined in the solution-treated or age-hardened condition, depending on the performance requirements of the end use.


Chemical, Physical, and Mechanical Properties of Inconel X-750

Inconel X-750 (UNS N07750 / AMS 5667 / ASTM B637) is supplied in multiple heat-treated conditions, including solution-annealed, age-hardened, or stress-equalized, for structural and fatigue-critical components.

Chemical Composition (Typical)

Element

Composition Range (wt.%)

Key Role

Nickel (Ni)

≥70.0

Base element; ensures high-temperature strength and corrosion resistance

Chromium (Cr)

14.0–17.0

Provides oxidation resistance and passivation stability

Iron (Fe)

5.0–9.0

Contributes to cost efficiency and structural toughness

Titanium (Ti)

2.25–2.75

Forms γ′ strengthening precipitates

Aluminum (Al)

0.40–1.0

Combines with Ti to enhance high-temp strength

Manganese (Mn)

≤1.0

Improves hot workability

Silicon (Si)

≤0.5

Enhances oxidation resistance

Copper (Cu)

≤0.5

Kept low to avoid corrosion risk

Carbon (C)

≤0.08

Controlled for ductility and weldability

Sulfur (S)

≤0.01

Minimized to prevent hot cracking

Niobium (Nb+Ta)

0.5–1.0

Promotes structural stability under stress


Physical Properties

Property

Value (Typical)

Test Standard/Condition

Density

8.28 g/cm³

ASTM B311

Melting Range

1390–1430°C

ASTM E1268

Thermal Conductivity

11.2 W/m·K at 100°C

ASTM E1225

Electrical Resistivity

1.25 µΩ·m at 20°C

ASTM B193

Thermal Expansion

13.3 µm/m·°C (20–1000°C)

ASTM E228

Specific Heat Capacity

460 J/kg·K at 20°C

ASTM E1269

Elastic Modulus

214 GPa at 20°C

ASTM E111


Mechanical Properties (Age-Hardened, AMS 5667)

Property

Value (Typical)

Test Standard

Tensile Strength

1000–1200 MPa

ASTM E8/E8M

Yield Strength (0.2%)

750–900 MPa

ASTM E8/E8M

Elongation

≥15% (25mm gauge)

ASTM E8/E8M

Hardness

320–370 HB

ASTM E10

Stress Rupture Strength

≥120 MPa @ 704°C, 1000h

ASTM E139


Key Characteristics of Inconel X-750

  • High Creep and Stress Rupture Resistance: Retains mechanical properties during extended exposure at 600–700°C, ideal for jet turbine and spring applications.

  • Excellent Oxidation and Corrosion Resistance: Resists chloride and sulfide attack, with proven performance in marine and nuclear environments.

  • Age-Hardenable Versatility: Mechanical properties can be tailored using solution annealing and aging treatments per application.

  • CNC Machinability: Requires careful tool control, but provides precision and stability for critical components with tolerances up to ±0.01 mm and Ra ≤ 1.0 µm.


CNC Machining Challenges and Solutions for Inconel X-750

Machining Challenges

High Work Hardening Rate

  • The alloy rapidly increases surface hardness during machining, leading to tool wear and dimensional inaccuracy if feeds and speeds are not optimized.

Abrasive Strengthening Phases

  • Precipitated γ′ and carbides (especially in aged condition) wear down tool edges and coatings, particularly in interrupted cuts.

Heat Retention

  • Low thermal conductivity concentrates heat at the cutting zone, necessitating high-pressure coolant and advanced tool materials.


Optimized Machining Strategies

Tool Selection

Parameter

Recommendation

Rationale

Tool Material

PVD-coated carbide or CBN tools

Withstand thermal fatigue and abrasive phases

Coating

AlTiN or TiSiN (2–5 µm)

Reduces friction and prolongs tool life

Geometry

10–12° rake, edge honed or chamfered

Improves chip evacuation and reduces cutting force

Cutting Parameters (ISO 3685)

Operation

Speed (m/min)

Feed (mm/rev)

DOC (mm)

Coolant Pressure (bar)

Roughing

20–30

0.20–0.30

2.0–3.0

80–100

Finishing

40–60

0.05–0.10

0.5–1.0

100–150


Surface Treatment for Machined Inconel X-750 Parts

Hot Isostatic Pressing (HIP)

HIP enhances creep rupture and fatigue resistance in cast or additively manufactured Inconel X-750 parts by eliminating porosity.

Heat Treatment

Heat Treatment includes solution annealing at 1095°C followed by aging at 705°C for 16–20 hours to optimize γ′ precipitation and tensile strength.

Superalloy Welding

Superalloy Welding employs GTAW with controlled heat input and Inconel X welding filler to reduce susceptibility to microcracking.

Thermal Barrier Coating (TBC)

TBC Coating applies 125–250 µm of YSZ to protect turbine rings and heat shields operating above 900°C.

Electrical Discharge Machining (EDM)

EDM enables precision slotting and profiling in hardened X-750 with tolerances up to ±0.01 mm.

Deep Hole Drilling

Deep Hole Drilling supports internal cooling passages in aerospace actuators and reactor spring systems with L/D ≥ 40:1.

Material Testing and Analysis

Material Testing includes stress rupture testing (ASTM E139), grain structure analysis (ASTM E112), and corrosion qualification (NACE, ASTM G28).


Industry Applications of Inconel X-750 Components

Aerospace

  • Turbine wheels, exhaust components, and jet engine springs.

  • Excellent thermal fatigue resistance under cyclic loads at 600–700°C.

Nuclear Reactors

  • Core springs, bolting, and structural supports.

  • Withstands neutron exposure and high-pressure steam corrosion.

Gas Turbines

  • Combustor hardware, transition ducts, and support brackets.

  • Maintains structural integrity and scale resistance under extreme heat.

Oil & Gas

  • Valve seats, downhole springs, and completion equipment.

  • Performs under hydrogen sulfide, chloride, and high-pressure cycling.