English

Inconel 738C

A cast nickel-based superalloy optimized for investment-cast, CNC-finished turbine components requiring thermal fatigue resistance, oxidation protection, and high-temperature mechanical performance.

Introduction to Inconel 738C

Inconel 738C is a cast nickel-based superalloy engineered for high-temperature structural applications where creep resistance, oxidation protection, and thermal fatigue resistance are critical. This alloy is an improved variant of Inconel 738, tailored for enhanced castability and better weldability, making it a reliable choice for precision-cast components that undergo CNC post-processing.

Inconel 738C retains a similar high γ′ content (~60%) and is stabilized by elements such as nickel (~62%), chromium (16%), cobalt (8.5–9.5%), titanium (3.4–3.8%), and aluminum (3.2–3.7%). It exhibits excellent high-temperature mechanical stability up to 980°C (1796°F), allowing its use in turbine vanes, combustor hardware, and other components exposed to aggressive thermal cycles.


Chemical, Physical, and Mechanical Properties of Inconel 738C

Inconel 738C (UNS R30738 / ASTM A297) is typically supplied in investment cast, solution heat-treated, and aged conditions, suitable for high-integrity aerospace and power turbine parts.

Chemical Composition (Typical Cast Analysis)

Element

Composition Range (wt.%)

Key Role

Nickel (Ni)

~62.0

Base matrix; high thermal strength

Chromium (Cr)

15.5–16.5

Oxidation and corrosion resistance

Cobalt (Co)

8.5–9.5

Enhances fatigue and thermal stability

Tungsten (W)

2.6–3.3

Solid-solution strength

Molybdenum (Mo)

1.5–2.1

Improves creep performance

Titanium (Ti)

3.4–3.8

γ′ formation for age-hardening

Aluminum (Al)

3.2–3.7

Combined with Ti to stabilize γ′ phase

Carbon (C)

0.08–0.12

Controlled for carbide formation and grain strength

Boron (B)

0.005–0.01

Improves ductility and crack resistance

Zirconium (Zr)

≤0.05

Increases grain boundary cohesion

Silicon (Si)

≤0.5

Enhances oxidation scale adherence

Manganese (Mn)

≤0.5

Aids castability and slag removal


Physical Properties

Property

Value (Typical)

Test Standard/Condition

Density

8.15 g/cm³

ASTM B311

Melting Range

1260–1330°C

ASTM E1268

Thermal Conductivity

11.0 W/m·K at 100°C

ASTM E1225

Electrical Resistivity

1.28 µΩ·m at 20°C

ASTM B193

Thermal Expansion

13.3 µm/m·°C (20–1000°C)

ASTM E228

Specific Heat Capacity

450 J/kg·K at 20°C

ASTM E1269

Elastic Modulus

188 GPa at 20°C

ASTM E111


Mechanical Properties (Cast + Aged Condition)

Property

Value (Typical)

Test Standard

Tensile Strength

980–1100 MPa

ASTM E8/E8M

Yield Strength (0.2%)

680–800 MPa

ASTM E8/E8M

Elongation

≥4–8% (25mm gauge)

ASTM E8/E8M

Hardness

330–390 HB

ASTM E10

Creep Rupture Strength

≥135 MPa @ 870°C, 1000h

ASTM E139


Key Characteristics of Inconel 738C

  • Optimized Castability: Improved fluidity and feeding behavior minimize shrinkage and porosity in complex turbine components.

  • High Gamma Prime Strength: γ′ volume fraction near 60% allows for excellent mechanical stability at high operating temperatures.

  • Surface Stability: Forms protective oxide scales (Cr₂O₃ and Al₂O₃) for superior oxidation resistance under cyclic heating conditions.

  • CNC Machining Readiness: Castings can be post-machined to tolerances of ±0.02 mm with surface finishes as fine as Ra ≤ 0.8 µm using high-performance tooling.


CNC Machining Challenges and Solutions for Inconel 738C

Machining Challenges

High Hardness

  • Age-hardened 738C parts can exceed 390 HB, creating difficulty in maintaining tool life and surface finish during extended machining cycles.

Heat Retention

  • Thermal conductivity under 12 W/m·K concentrates heat at the cutting zone, requiring advanced cooling and coating solutions.

Microstructural Abrasiveness

  • Intermetallic phases and carbides contribute to rapid edge wear and crater formation, especially at high cutting speeds.


Optimized Machining Strategies

Tool Selection

Parameter

Recommendation

Rationale

Tool Material

SiAlON ceramics or PVD-coated carbide

Withstands extreme heat and abrasive wear

Coating

TiAlN, AlCrN (3–6 µm thickness)

Reduces thermal load and friction

Geometry

10–12° positive rake, edge-prepped insert

Controls cutting forces and delays edge failure

Cutting Parameters (ISO 3685)

Operation

Speed (m/min)

Feed (mm/rev)

DOC (mm)

Coolant Pressure (bar)

Roughing

15–25

0.20–0.30

2.0–3.0

80–100

Finishing

30–45

0.05–0.10

0.3–0.8

100–150


Surface Treatment for Machined Inconel 738C Parts

Hot Isostatic Pressing (HIP)

HIP densifies internal microstructures and improves low-cycle fatigue resistance by eliminating microporosity typical in castings.

Heat Treatment

Heat Treatment involves solutioning at 1120–1170°C followed by aging at 845°C to fully precipitate the γ′ phase for strength and thermal stability.

Superalloy Welding

Superalloy Welding is possible with preheating and controlled filler metal application, minimizing cracking during joining or repair.

Thermal Barrier Coating (TBC)

TBC Coating applies 125–250 µm of YSZ ceramics to extend thermal fatigue life and reduce in-service oxidation of airfoil surfaces.

Electrical Discharge Machining (EDM)

EDM enables precise cutting of cooling slots, fir-tree roots, and complex features to ±0.01 mm accuracy post-casting.

Deep Hole Drilling

Deep Hole Drilling provides accurate, high-aspect-ratio holes (L/D ≥ 40:1) essential for cooling flow channels in turbine applications.

Material Testing and Analysis

Material Testing includes microstructural analysis, tensile/corrosion testing, and NDT per ASTM E139, E112, and AMS 5389 standards.


Industry Applications of Inconel 738C Components

Aircraft Turbines

  • Nozzle guide vanes, turbine blades, and shroud segments.

  • Delivers mechanical integrity at 900–980°C under cyclic flight conditions.

Industrial Gas Turbines

  • Transition ducts, combustor parts, and rotor segments.

  • Performs under high-pressure combustion and rapid thermal cycling.

Power & Energy

  • Turbine exhaust frames, seals, and heat shield systems.

  • Combines oxidation resistance with long-term creep strength.

Defense & Space Propulsion

  • High-temperature jet engine and rocket nozzle components.

  • Maintains load-bearing strength in harsh reentry and launch environments.