Hastelloy C-276 is a corrosion-resistant nickel-molybdenum-chromium alloy engineered for use in the most aggressive chemical environments. It offers excellent resistance to strong oxidizers, reducing agents, and both organic and inorganic acids—especially hydrochloric acid, sulfuric acid, and wet chlorine. The alloy's low carbon content also minimizes the risk of grain boundary precipitation during welding, preserving its corrosion resistance in welded structures.
Hastelloy C-276 is widely used in CNC-machined components that operate under severe conditions, such as flue gas scrubbers, heat exchangers, and pollution control systems. Its unique thermal stability, corrosion resistance, and mechanical strength make it a top-tier material for chemical processing and marine industries.
Hastelloy C-276 (UNS N10276 / ASTM B575 / B619 / B622 / B626) is a versatile superalloy that maintains structural and chemical stability in highly corrosive media.
Element | Composition Range (wt.%) | Key Role |
|---|---|---|
Nickel (Ni) | Balance (≥57.0) | Base metal for corrosion resistance and strength |
Molybdenum (Mo) | 15.0–17.0 | Improves resistance to reducing acids and pitting |
Chromium (Cr) | 14.5–16.5 | Forms passive oxide layers to resist oxidizers |
Iron (Fe) | 4.0–7.0 | Enhances mechanical properties |
Tungsten (W) | 3.0–4.5 | Boosts localized corrosion resistance |
Cobalt (Co) | ≤2.5 | Minor alloying element |
Carbon (C) | ≤0.01 | Prevents carbide precipitation in weld zones |
Manganese (Mn) | ≤1.0 | Improves hot formability |
Silicon (Si) | ≤0.08 | Minimizes intergranular attack |
Sulfur (S) | ≤0.03 | Controlled to reduce cracking during machining |
Vanadium (V) | ≤0.35 | Enhances microstructural stability |
Property | Value (Typical) | Test Standard/Condition |
|---|---|---|
Density | 8.89 g/cm³ | ASTM B311 |
Melting Range | 1325–1370°C | ASTM E1268 |
Thermal Conductivity | 10.5 W/m·K at 100°C | ASTM E1225 |
Electrical Resistivity | 1.20 µΩ·m at 20°C | ASTM B193 |
Thermal Expansion | 11.2 µm/m·°C (20–300°C) | ASTM E228 |
Specific Heat Capacity | 420 J/kg·K at 20°C | ASTM E1269 |
Elastic Modulus | 205 GPa at 20°C | ASTM E111 |
Property | Value (Typical) | Test Standard |
|---|---|---|
Tensile Strength | 760–825 MPa | ASTM E8/E8M |
Yield Strength (0.2%) | 280–355 MPa | ASTM E8/E8M |
Elongation | ≥40% (25mm gauge) | ASTM E8/E8M |
Hardness | 190–230 HB | ASTM E10 |
Impact Toughness | Excellent across sub-zero to elevated temperatures | ASTM E23 |
Exceptional Acid Resistance: Corrosion rates <0.02 mm/year in boiling hydrochloric acid (up to 37%), sulfuric acid, and formic acid mixtures.
Weldability: Low carbon and silicon contents prevent sensitization and intergranular attack during welding or post-weld heat treatment.
Thermal and Oxidation Stability: Withstands continuous service up to 1040°C in oxidizing and sulfur-laden atmospheres.
Precision Machinability: Maintains dimensional tolerances to ±0.01 mm and surface finishes <Ra 0.8 µm with proper tooling and coolant strategies.
High molybdenum content promotes strain hardening during shallow cuts or interrupted machining, increasing tool wear.
Heat retention due to low thermal conductivity causes flank wear and edge chipping in uncoated tools.
BUE (Built-Up Edge) formation can occur without high-pressure coolant and polished tool surfaces.
Parameter | Recommendation | Rationale |
|---|---|---|
Tool Material | Carbide (K20–K30) or ceramic inserts | High-temperature wear resistance |
Coating | AlTiN or AlCrN PVD coating (3–5 µm) | Improves heat resistance and chip flow |
Geometry | Positive rake (8–12°), honed edge radius 0.02–0.05 mm | Minimizes cutting force and work hardening |
Operation | Speed (m/min) | Feed (mm/rev) | DOC (mm) | Coolant Pressure (bar) |
|---|---|---|---|---|
Roughing | 12–18 | 0.20–0.30 | 2.0–3.5 | 100–120 |
Finishing | 20–30 | 0.05–0.10 | 0.5–1.0 | 120–150 |
HIP at 1150°C and 100–200 MPa eliminates shrinkage porosity and improves fatigue resistance by ≥20%.
Heat Treatment includes solution annealing at 1120–1175°C followed by rapid quenching to prevent secondary phase formation.
Superalloy Welding with ERNiCrMo-4 filler ensures corrosion-resistant weld zones with low interpass temperatures (<150°C).
TBC Coating provides insulation for parts exposed to 900–1050°C and acidic or SO₂-rich environments.
EDM supports fine-feature profiling with tolerances of ±0.005 mm and Ra <0.6 µm.
Deep Hole Drilling enables high-precision drilling at L/D ratios >30:1 for reactor tubing and chemical processing manifolds.
Material Testing includes G28 and A262 corrosion testing, mechanical validation (E8, E18), and metallography.
Heat exchangers, scrubber systems, and digesters in oxidizing-reducing acid environments.
Ducting, fans, and absorber towers exposed to wet chlorine gas and acidic condensate at elevated temperatures.
Valve components, pump housings, and offshore riser tubes resistant to biofouling and seawater corrosion.
Pressure vessels and agitators handling nitric, hydrochloric, and sulfuric acid mixtures with organics.