English

Hastelloy B-2

A nickel-molybdenum superalloy designed for superior performance in reducing acid environments. Enhanced with low iron and carbon for improved weldability, CNC machinability, and corrosion resistance in chemical process systems.

Introduction to Hastelloy B-2

Hastelloy B-2 is a wrought, nickel-molybdenum alloy engineered to resist strong reducing agents, particularly hydrochloric acid. As an improved version of Hastelloy B, it offers greater thermal stability, better weldability, and reduced susceptibility to stress corrosion cracking and knife-line attack in heat-affected zones.

The alloy’s optimized composition, with minimized iron and carbon content, ensures superior corrosion resistance in chemical processing environments. Hastelloy B-2 is frequently CNC machined into components such as heat exchanger parts, pump housings, and acid handling equipment where structural integrity and chemical compatibility are essential.


Chemical, Physical, and Mechanical Properties of Hastelloy B-2

Hastelloy B-2 (UNS N10665 / ASTM B333 / B335) is a solid-solution strengthened nickel-molybdenum alloy with refined impurity control. It maintains structural stability across a wide temperature range and is typically used in the annealed condition for optimal performance.

Chemical Composition (Typical)

Element

Composition Range (wt.%)

Key Role

Nickel (Ni)

Balance (≥65.0)

Base element; ensures corrosion resistance in reducing media

Molybdenum (Mo)

26.0–30.0

Improves pitting and crevice corrosion resistance

Iron (Fe)

≤2.0

Controlled to enhance corrosion resistance and stability

Carbon (C)

≤0.01

Prevents carbide precipitation in heat-affected zones

Manganese (Mn)

≤1.0

Improves hot workability

Silicon (Si)

≤0.1

Reduced to mitigate intergranular corrosion

Cobalt (Co)

≤1.0

Limited as an impurity

Chromium (Cr)

≤1.0

Kept low to avoid compromising performance in reducing environments

Sulfur (S)

≤0.02

Minimized to prevent hot cracking during processing


Physical Properties

Property

Value (Typical)

Test Standard/Condition

Density

9.22 g/cm³

ASTM B311

Melting Range

1330–1380°C

ASTM E1268

Thermal Conductivity

10.5 W/m·K at 100°C

ASTM E1225

Electrical Resistivity

1.25 µΩ·m at 20°C

ASTM B193

Thermal Expansion

12.2 µm/m·°C (20–300°C)

ASTM E228

Specific Heat Capacity

395 J/kg·K at 20°C

ASTM E1269

Elastic Modulus

200 GPa at 20°C

ASTM E111


Mechanical Properties (Annealed Condition)

Property

Value (Typical)

Test Standard

Tensile Strength

690–760 MPa

ASTM E8/E8M

Yield Strength (0.2%)

275–345 MPa

ASTM E8/E8M

Elongation

≥40% (25mm gauge)

ASTM E8/E8M

Hardness

180–220 HB

ASTM E10

Impact Toughness

Excellent at cryogenic and ambient conditions

ASTM E23


Key Characteristics of Hastelloy B-2

  • Superior Acid Resistance: Offers corrosion rates <0.01 mm/year in boiling 20% hydrochloric acid, outperforming many high-nickel alloys in reducing environments.

  • Weldability Improvements: Unlike Hastelloy B, Hastelloy B-2 is less prone to weld-related intergranular attack due to reduced C, Si, and Fe content.

  • Thermal Stability: Resists phase separation and maintains corrosion resistance after thermal cycling between 425–870°C.

  • CNC-Friendly Annealed Structure: Consistent grain size and ductility aid in achieving fine finishes and tight tolerances (<±0.01 mm) in machined parts.


CNC Machining Challenges and Solutions for Hastelloy B-2

Machining Challenges

Work Hardening

  • Surface hardness may increase by 30–40% during cutting if feed rates are too low, leading to excessive tool wear.

Heat Generation

  • Low thermal conductivity causes cutting zone temperatures to exceed 600°C, necessitating coolant optimization.

Tool Adhesion

  • High nickel content promotes chip adhesion and built-up edge formation on standard inserts.


Optimized Machining Strategies

Tool Selection

Parameter

Recommendation

Rationale

Tool Material

PVD-coated carbide (ISO K20–K30) or ceramic inserts

High wear resistance under thermal loads

Coating

AlTiN or AlCrN (3–5 µm)

Reduces heat absorption and chip adhesion

Geometry

Positive rake (10–15°), honed edges (0.02–0.04 mm radius)

Enhances chip flow and surface finish

Cutting Parameters (ISO 3685)

Operation

Speed (m/min)

Feed (mm/rev)

DOC (mm)

Coolant Pressure (bar)

Roughing

10–20

0.20–0.30

2.0–3.0

90–120

Finishing

20–35

0.05–0.10

0.5–1.0

120–150


Surface Treatment for Machined Hastelloy B-2 Parts

Hot Isostatic Pressing (HIP)

HIP improves fatigue life and eliminates porosity in critical cast or additive parts.

Heat Treatment

Heat Treatment involves annealing at 1065°C ±10°C followed by rapid quenching to retain corrosion resistance.

Superalloy Welding

Superalloy Welding utilizes GTAW with ERNiMo-7 filler to minimize phase segregation and ensure corrosion resistance in the weld zone.

Thermal Barrier Coating (TBC)

TBC Coating can be applied to extend component life in mixed-phase or acid vapor environments.

Electrical Discharge Machining (EDM)

EDM enables non-contact machining of tight-tolerance geometries in heat exchanger plates or fittings.

Deep Hole Drilling

Deep Hole Drilling supports L/D up to 30:1 for reactor tubing, acid distributor ports, and internal channeling.

Material Testing and Analysis

Material Testing includes corrosion testing (ASTM G28 Method A), metallographic evaluation (ASTM E3), and mechanical validation (ASTM E8, E18).


Industry Applications of Hastelloy B-2 Components

Chemical Processing

  • Pump bodies, impellers, and acid nozzles for HCl-rich environments.

  • Maintains <0.05 mm/year corrosion rates even at 90°C in reducing acid flows.

Pharmaceutical Reactors

  • Mixing shafts, liners, and vessels exposed to high-purity reducing agents.

  • Prevents contamination and pitting from chlorides and sulfides.

Pickling and Acid Regeneration

  • Components in HF, HCl, and sulfuric acid recovery lines.

  • Withstands multi-phase flows and rapid thermal cycling.

Metal Finishing

  • Heater elements and anodes exposed to strong acid baths.

  • Maintains mechanical integrity under long-term immersion.


Explore Related Blogs