Rene 142

A nickel-based superalloy designed for use in high-temperature, high-performance applications such as gas turbines and combustion systems. Rene 142 provides superior strength, oxidation resistance, and weldability, making it ideal for precision CNC machining in aerospace, power generation, and industrial applications.

Introduction to Rene 142

Rene 142 is a high-performance nickel-based superalloy known for its exceptional strength, oxidation resistance, and stability at high temperatures. It is widely used in demanding applications, particularly in aerospace and power generation, where components experience extreme mechanical and thermal stress. Rene 142’s unique composition enables it to retain its structural integrity at temperatures exceeding 1000°C, making it ideal for turbine blades, engine components, and high-efficiency power systems.

Due to the precise manufacturing requirements of these applications, CNC machining services are essential for producing Rene 142 components. CNC machining allows manufacturers to achieve tight tolerances and ensure optimal performance in critical aerospace and industrial parts.


Chemical, Physical, and Mechanical Properties of Rene 142

Rene 142 (UNS N07042 / W.Nr. 2.4956) is a nickel-chromium-aluminum alloy designed for maximum strength, oxidation resistance, and long-term creep resistance at elevated temperatures, making it ideal for turbine and combustion system components.

Chemical Composition (Typical)

Element

Composition Range (wt.%)

Key Role

Nickel (Ni)

Balance (~55.0)

Base matrix; provides high-temperature strength and corrosion resistance

Chromium (Cr)

13.0–15.0

Forms Cr₂O₃ oxide layer, providing oxidation resistance at high temperatures

Cobalt (Co)

8.0–10.0

Enhances high-temperature strength and resistance to thermal fatigue

Molybdenum (Mo)

2.5–3.5

Solid solution strengthening to increase creep and fatigue resistance

Titanium (Ti)

3.0–4.0

Forms γ′ phase for precipitation hardening, increasing strength

Aluminum (Al)

2.5–3.5

Forms the γ′ phase, enhancing creep resistance and tensile strength

Iron (Fe)

≤1.0

Residual element

Carbon (C)

≤0.08

Improves strength at high temperatures by forming carbides

Manganese (Mn)

≤1.0

Enhances hot workability and reduces carbide formation

Silicon (Si)

≤0.5

Improves oxidation resistance and high-temperature stability

Boron (B)

≤0.005

Increases grain boundary strength, improving creep resistance

Zirconium (Zr)

≤0.05

Increases creep rupture strength and stability at elevated temperatures


Physical Properties

Property

Value (Typical)

Test Standard/Condition

Density

8.4 g/cm³

ASTM B311

Melting Range

1320–1370°C

ASTM E1268

Thermal Conductivity

13.5 W/m·K at 100°C

ASTM E1225

Electrical Resistivity

1.15 µΩ·m at 20°C

ASTM B193

Thermal Expansion

14.2 µm/m·°C (20–1000°C)

ASTM E228

Specific Heat Capacity

460 J/kg·K at 20°C

ASTM E1269

Elastic Modulus

215 GPa at 20°C

ASTM E111


Mechanical Properties (Solution Treated + Aged)

Property

Value (Typical)

Test Standard

Tensile Strength

1050–1250 MPa

ASTM E8/E8M

Yield Strength (0.2%)

750–900 MPa

ASTM E8/E8M

Elongation

≥20%

ASTM E8/E8M

Hardness

240–270 HB

ASTM E10

Creep Rupture Strength

210 MPa at 900°C (1000h)

ASTM E139

Fatigue Resistance

Excellent

ASTM E466


Key Characteristics of Rene 142

  • High-Temperature Strength and Durability Rene 142 retains tensile strength up to 1050 MPa at 850–900°C, making it highly suitable for high-stress environments such as gas turbine engines and combustion systems.

  • Precipitation Strengthening The γ′ phase formed during aging treatment increases the alloy’s tensile strength and resistance to thermal fatigue, making it ideal for components subjected to thermal cycling.

  • Oxidation and Corrosion Resistance Rene 142’s chromium and aluminum content enables the formation of a stable protective oxide layer, providing resistance to oxidation and corrosion up to 1050°C in high-pressure environments.

  • Creep and Fatigue Resistance With a creep rupture strength of over 210 MPa at 900°C, Rene 142 excels in long-term high-temperature applications, preventing dimensional changes under sustained mechanical stress.

  • Weldability Rene 142 exhibits good weldability with minimal strength degradation in the heat-affected zone, allowing for easy fabrication and repair of critical components.


CNC Machining Challenges and Solutions for Rene 142

Machining Challenges

Tool Wear and Edge Chipping

  • The high hardness and solid solution strengthening phases in Rene 142 increase the wear on carbide tools during machining, especially under aggressive cutting conditions.

Heat Generation

  • The low thermal conductivity of Rene 142 leads to high cutting temperatures, which can cause thermal distortion and reduce tool life unless cooling is applied effectively.

Work Hardening

  • The material's work hardening tendency means that cutting forces increase during machining, which can result in surface hardness exceeding the desired range if not carefully controlled.


Optimized Machining Strategies

Tool Selection

Parameter

Recommendation

Rationale

Tool Material

Carbide (K20–K30) or CBN inserts for finishing

Resists wear and maintains sharpness under high cutting temperatures

Coating

AlTiN or TiSiN PVD (3–5 µm)

Reduces friction and heat buildup

Geometry

Positive rake angle (6–8°), sharp cutting edge (~0.05 mm)

Minimizes cutting forces and prevents excessive tool wear

Cutting Parameters (ISO 3685 Compliant)

Operation

Speed (m/min)

Feed (mm/rev)

Depth of Cut (mm)

Coolant Pressure (bar)

Roughing

12–20

0.15–0.25

2.0–3.0

100–120

Finishing

25–35

0.05–0.10

0.3–0.8

120–150


Surface Treatment for Machined Rene 142 Parts

Hot Isostatic Pressing (HIP)

HIP reduces internal porosity and enhances fatigue strength by >25%, ensuring reliability in critical turbine and aerospace components.

Heat Treatment

Heat Treatment involves solution treatment at 1100°C followed by aging at 800°C to optimize the formation of γ′ precipitates, improving creep resistance and tensile strength.

Superalloy Welding

Superalloy Welding provides strong, crack-free welds with minimal loss of mechanical properties, ensuring high-performance components can be repaired without degradation.

Thermal Barrier Coating (TBC)

TBC Coating improves the durability of turbine blades by reducing surface temperatures by up to 250°C, extending the component's service life under extreme thermal cycling.

Electrical Discharge Machining (EDM)

EDM allows the creation of intricate internal features such as high-precision cooling holes and microchannels, achieving tolerances as tight as ±0.005 mm.

Deep Hole Drilling

Deep Hole Drilling ensures precision in deep, high-accuracy passages needed for gas turbine components, with concentricity deviations of less than 0.3 mm/m.

Material Testing and Analysis

Material Testing includes tensile, creep, and fatigue testing to validate the material's performance at high temperatures and X-ray diffraction to assess the γ′ phase distribution.


Industry Applications of Rene 142 Components

  • Aerospace Turbine Engines: Turbine blades, compressor discs, and nozzles exposed to cyclic thermal and mechanical stresses.

  • Power Generation: Gas turbine components such as blades, vanes, and nozzles are used in high-efficiency turbines.

  • Nuclear Reactors: Reactor core components, pressure vessels, and heat exchangers subjected to high radiation and thermal stresses.

  • Automotive Turbo Systems: Exhaust valves, turbocharger wheels, and heat-resistant engine parts for high-performance vehicles.

  • Industrial Heat Treatment Equipment: Furnace parts, seals, and fixtures that require excellent resistance to high temperatures.


FAQs

  1. What are the machining challenges when processing Rene 142 for aerospace turbine components?

  2. How does heat treatment enhance the high-temperature performance of Rene 142 parts?

  3. What are the best surface treatments for Rene 142 to improve its resistance to thermal cycling?

  4. How does Rene 142’s workability compare to other superalloys for high-temperature applications?

  5. What material testing is essential for ensuring the reliability of Rene 142 components in critical aerospace applications?

Explorer les blogs associés